GC1115 insert grade
GC1115 is Sandvik’s PVD-coated carbide grade (PVD) for ISO M05–M25 and S15–S25, as Sandvik’s catalog prints it. Stainless at low feed or medium speed; superalloys and titanium with sharp edges, medium to rough turning of smearing materials.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- PVD-coated carbide
- Coating
- PVD
- ISO M
- M05–M25 (core M15) · stainless steel
- ISO S
- S15–S25 (core S20) · superalloys and titanium
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
GC1115 equivalents by material
Stainless · M
Read at M15, the centre of Sandvik’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | M05–M20 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | M10–M30 (core M20) | One source: Mitsubishi Materials, its own catalog |
| Seco | CP500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M10–M30 | One source: Seco Tools, its own catalog |
Why GC1115 for austenitic stainless (304, 316)
GC1115 for austenitic stainless (304, 316): rated M05–M25 (core M15) by Sandvik.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Sandvik rates GC1115 (PVD-coated carbide) for M05–M25 (core M15): Stainless at low feed or medium speed; superalloys and titanium with sharp edges, medium to rough turning of smearing materials.
One source: Sandvik Coromant, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
Superalloys · S
Read at S20, the centre of Sandvik’s S range (superalloys and titanium). Each grade is one its own maker rates for S20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC806 | PVD-coated carbide | PVD, AlTiN (SUMOTEC treated) | S15–S25 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about S10–S20 | One source: Seco Tools, its own catalog |
Why GC1115 for heat-resistant superalloys (Inconel 718)
GC1115 for heat-resistant superalloys (Inconel 718): rated S15–S25 (core S20) by Sandvik.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Sandvik rates GC1115 (PVD-coated carbide) for S15–S25 (core S20): Stainless at low feed or medium speed; superalloys and titanium with sharp edges, medium to rough turning of smearing materials.
One source: Sandvik Coromant, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC1115 at M10, M20. Sandvik Coromant’s own catalog is the authority for its grade.
It agrees with Sandvik Coromant’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)