Kennametal · PVD-coated carbide
KC5410 insert grade
KC5410 is Kennametal’s PVD-coated carbide grade (PVD, TiB2) for ISO N05–N20, as Kennametal’s catalog prints it. Aluminum (under 12.2% Si) and magnesium alloys; the coating resists built-up edge.
One source: Kennametal, its own catalog
What Kennametal prints
- Type
- PVD-coated carbide
- Coating
- PVD, TiB2
- Substrate
- Very deformation-resistant, fine-grain unalloyed carbide
- ISO N
- N05–N20 · non-ferrous
- Operations
- turning
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
KC5410 equivalents by material
ISO N (non-ferrous)
Read at N15, the centre of Kennametal’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC907 | PVD-coated carbide | PVD, TiAlN | N05–N20 | One source: ISCAR, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why KC5410 for aluminum
KC5410 for aluminum: rated N05–N20 by Kennametal.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Kennametal rates KC5410 (PVD-coated carbide) for N05–N20: Aluminum (under 12.2% Si) and magnesium alloys; the coating resists built-up edge.
One source: Kennametal, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists KC5410 at S10. Kennametal’s own catalog is the authority for its grade.
- The cross-reference lists S10; Kennametal gives no S application (its range: N05–N20).
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)