Insert grades · Kennametal
Kennametal insert grade chart
12 Kennametal insert grades, each as Kennametal’s own catalog prints it: 4 CVD-coated carbide, 6 PVD-coated carbide and 2 uncoated carbide. The table gives each grade’s coating and ISO range; each page lists the other makers’ grades for the same class.
One source: Kennametal, its own catalog
Kennametal insert grades by type
| Grade | Type | Coating | ISO range |
|---|---|---|---|
| KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P20–P25 and M10–M20 |
| KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 and M20–M30 |
| KCM35 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P40–P45 and M30–M40 |
| KCP40 | CVD-coated carbide | CVD, Thin MTCVD TiCN-Al2O3 | P35–P45 and M20–M30 |
| KC5010 | PVD-coated carbide | PVD, AlTiN | P10–P20, M10–M20, K05–K20, N10–N20, S10–S20 and H10–H10 |
| KC5025 | PVD-coated carbide | PVD, AlTiN | P20–P30, M20–M30, K20–K30, N20–N30 and S20–S30 |
| KC5410 | PVD-coated carbide | PVD, TiB2 | N05–N20 |
| KCS10 | PVD-coated carbide | PVD, AlTiN | P10–P20, M10–M20, K05–K20, N10–N20, S10–S20 and H10–H10 |
| KCU10 | PVD-coated carbide | PVD, Multilayer | P10–P20, M10–M20, K05–K20, N10–N20, S10–S20 and H10–H10 |
| KCU25 | PVD-coated carbide | PVD, AlTiN | P20–P30, M20–M30, K20–K30, N20–N30 and S20–S30 |
| K68 | uncoated carbide | Uncoated | M10–M20, K05–K20, N10–N20 and S10–S20 |
| K313 | uncoated carbide | Uncoated | M10–M20, K05–K20, N10–N20 and S10–S20 |