Mitsubishi · CVD-coated carbide
MC5005 insert grade
MC5005 is Mitsubishi’s CVD-coated carbide grade (CVD) for ISO K01–K20, as Mitsubishi’s catalog prints it. Cast iron, continuous cutting; Mitsubishi’s first choice for light cutting in stable conditions.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- CVD-coated carbide
- Coating
- CVD
- ISO K
- K01–K20 (core K10) · cast iron
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names MC5005 its first choice for gray cast iron, up to 350 MPa (e.g. Class 45 B), stable conditions: finishing.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerMC5005 equivalents by material
ISO K (cast iron)
Read at K10, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC20 | uncoated carbide | Uncoated | K10–K20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | K05–K20 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why MC5005 for gray cast iron
MC5005 for gray cast iron: rated K01–K20 (core K10) by Mitsubishi.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
Mitsubishi rates MC5005 (CVD-coated carbide) for K01–K20 (core K10): Cast iron, continuous cutting; Mitsubishi’s first choice for light cutting in stable conditions.
One source: Mitsubishi Materials, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO K cast iron
- Mitsubishi Materials — Machining course: ISO group K, cast iron
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists MC5005 at K01. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)