ISCAR · uncoated carbide
IC20 insert grade
IC20 is ISCAR’s uncoated carbide grade (Uncoated) for ISO M10–M25, K10–K20, N05–N25, S05–S20 and H05–H15, as ISCAR’s catalog prints it. Semi-finishing to semi-roughing of aluminum, cast iron and stainless.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- uncoated carbide
- Coating
- Uncoated
- ISO M
- M10–M25 · stainless steel
- ISO K
- K10–K20 · cast iron
- ISO N
- N05–N25 · non-ferrous
- ISO S
- S05–S20 · superalloys and titanium
- ISO H
- H05–H15 · hardened steel
- Operations
- turning, milling
IC20 equivalents by material
Stainless · M
Read at M20, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | US7020 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M10–M30 (core M20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2220 | CVD-coated carbide | Coated (process not printed) | M15–M30 (core M20) | One source: Sandvik Coromant, its own catalog |
| Seco | CP500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M10–M30 | One source: Seco Tools, its own catalog |
Why IC20 for austenitic stainless (304, 316)
IC20 for austenitic stainless (304, 316): rated M10–M25 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC20 (uncoated carbide) for M10–M25: Semi-finishing to semi-roughing of aluminum, cast iron and stainless.
One source: ISCAR, the maker of the grade , sources [4]
Cast iron · K
Read at K15, the centre of ISCAR’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | K05–K20 | One source: Kennametal, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | K10–K20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why IC20 for gray cast iron
IC20 for gray cast iron: rated K10–K20 by ISCAR.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC20 (uncoated carbide) for K10–K20: Semi-finishing to semi-roughing of aluminum, cast iron and stainless.
One source: ISCAR, the maker of the grade , sources [3]
Non-ferrous · N
Read at N15, the centre of ISCAR’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | N10–N20 | One source: Kennametal, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why IC20 for aluminum
IC20 for aluminum: rated N05–N25 by ISCAR.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC20 (uncoated carbide) for N05–N25: Semi-finishing to semi-roughing of aluminum, cast iron and stainless.
One source: ISCAR, the maker of the grade , sources [3]
Superalloys · S
Read at S15, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MT9015 | uncoated carbide | Uncoated | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | S10–S30 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | HX | uncoated carbide | Uncoated | about S10–S25 | One source: Seco Tools, its own catalog |
Why IC20 for heat-resistant superalloys (Inconel 718)
IC20 for heat-resistant superalloys (Inconel 718): rated S05–S20 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC20 (uncoated carbide) for S05–S20: Semi-finishing to semi-roughing of aluminum, cast iron and stainless.
One source: ISCAR, the maker of the grade , sources [4]
Hardened · H
Read at H10, the centre of ISCAR’s H range (hardened steel). Each grade is one its own maker rates for H10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | H10–H10 | One source: Kennametal, its own catalog |
| Seco | TH1000 | PVD-coated carbide | PVD, Ti-Al-Si-N nanolaminate | about H05–H15 | One source: Seco Tools, its own catalog |
Why IC20 for hardened steel
IC20 for hardened steel: rated H05–H15 by ISCAR.
The reasoning, step by step
The situation
Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC20 (uncoated carbide) for H05–H15: Semi-finishing to semi-roughing of aluminum, cast iron and stainless.
One source: ISCAR, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC20 at M20, M30, K10, K20, N10, N20. ISCAR’s own catalog is the authority for its grade.
- The cross-reference lists M30; ISCAR gives M10–M25.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)