Sandvik · uncoated carbide

H13A insert grade

H13A is Sandvik’s uncoated carbide grade (Uncoated) for ISO K10–K30, N05–N25 and S10–S30, as Sandvik’s catalog prints it. Basic grade for titanium alloys and a superalloy grade for moderate to low speeds; also cast iron and aluminum.

One source: Sandvik Coromant, its own catalog

The cutting edge of a uncoated carbide insert in section: the carbide substrate, uncoated; rated for ISO K, N and S.cutting edgesubstrate carbideISO groupKNS
The edge in section; its ISO groups. Not to scale.

What Sandvik prints

Type
uncoated carbide
Coating
Uncoated
ISO K
K10–K30 (core K20) · cast iron
ISO N
N05–N25 (core N15) · non-ferrous
ISO S
S10–S30 (core S15) · superalloys and titanium
Operations
turning

Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

H13A equivalents by material

Cast iron · K

Read at K20, the centre of Sandvik’s K range (cast iron). Each grade is one its own maker rates for K20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K20
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC20uncoated carbideUncoatedK10–K20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedK05–K20

One source: Kennametal, its own catalog

MitsubishiHTi10uncoated carbideUncoatedK10–K20

One source: Mitsubishi Materials, its own catalog

Why H13A for gray cast iron

H13A for gray cast iron: rated K10–K30 (core K20) by Sandvik.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Sandvik rates H13A (uncoated carbide) for K10–K30 (core K20): Basic grade for titanium alloys and a superalloy grade for moderate to low speeds; also cast iron and aluminum.

    One source: Sandvik Coromant, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

Non-ferrous · N

Read at N15, the centre of Sandvik’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for N15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC08uncoated carbideUncoatedN10–N20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedN10–N20

One source: Kennametal, its own catalog

MitsubishiHTi10uncoated carbideUncoatedN10–N20

One source: Mitsubishi Materials, its own catalog

Why H13A for aluminum

H13A for aluminum: rated N05–N25 (core N15) by Sandvik.

The reasoning, step by step
  1. The situation

    Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    It wants a sharp edge with low cutting force, one chips don’t weld to.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  3. So

    Sandvik rates H13A (uncoated carbide) for N05–N25 (core N15): Basic grade for titanium alloys and a superalloy grade for moderate to low speeds; also cast iron and aluminum.

    One source: Sandvik Coromant, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO N non-ferrous
  2. Mitsubishi Materials — Machining course: ISO group N, non-ferrous metals
  3. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

Superalloys · S

Read at S15, the centre of Sandvik’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC20uncoated carbideUncoatedS05–S20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedS10–S20

One source: Kennametal, its own catalog

MitsubishiMT9015uncoated carbideUncoatedS05–S25 (core S15)

One source: Mitsubishi Materials, its own catalog

SecoHXuncoated carbideUncoatedabout S10–S25

One source: Seco Tools, its own catalog

Why H13A for heat-resistant superalloys (Inconel 718)

H13A for heat-resistant superalloys (Inconel 718): rated S10–S30 (core S15) by Sandvik.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Sandvik rates H13A (uncoated carbide) for S10–S30 (core S15): Basic grade for titanium alloys and a superalloy grade for moderate to low speeds; also cast iron and aluminum.

    One source: Sandvik Coromant, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists H13A at M20, K20, N01, S10. Sandvik Coromant’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)