Mitsubishi · CVD-coated carbide

MC5115 insert grade

MC5115 is Mitsubishi’s CVD-coated carbide grade (CVD, TiCN-Al2O3, thick) for ISO K05–K25, as Mitsubishi’s catalog prints it. Cast iron and ductile cast iron, interrupted cutting; layers that resist peeling on ductile iron.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO K.cutting edgecoating CVDsubstrate carbideISO groupK
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Mitsubishi prints

Type
CVD-coated carbide
Coating
CVD, TiCN-Al2O3, thick
Substrate
91.0 HRA
ISO K
K05–K25 (core K15) · cast iron
Operations
turning

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

Mitsubishi’s first choice

  • Mitsubishi names MC5115 its first choice for gray cast iron, up to 350 MPa (e.g. Class 45 B), unstable conditions: finishing, medium and roughing.

One source: Mitsubishi Materials, its own catalog

Open the insert picker

MC5115 equivalents by material

ISO K (cast iron)

Read at K15, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC20uncoated carbideUncoatedK10–K20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedK05–K20

One source: Kennametal, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why MC5115 for gray cast iron

MC5115 for gray cast iron: rated K05–K25 (core K15) by Mitsubishi.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.

    Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]

  3. So

    Mitsubishi rates MC5115 (CVD-coated carbide) for K05–K25 (core K15): Cast iron and ductile cast iron, interrupted cutting; layers that resist peeling on ductile iron.

    One source: Mitsubishi Materials, the maker of the grade , sources [5]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  4. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  5. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)