Mitsubishi · CVD-coated carbide
US7020 insert grade
US7020 is Mitsubishi’s CVD-coated carbide grade (CVD, TiCN-Al2O3-TiN, thin) for ISO M10–M30, as Mitsubishi’s catalog prints it. Stainless steel, continuous to light interrupted cutting.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- CVD-coated carbide
- Coating
- CVD, TiCN-Al2O3-TiN, thin
- Substrate
- 90.5 HRA
- ISO M
- M10–M30 (core M20) · stainless steel
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
US7020 equivalents by material
ISO M (stainless steel)
Read at M20, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC9350 | CVD-coated carbide | CVD, TiCN + alpha Al2O3 + TiN | M15–M30 | One source: ISCAR, its own catalog |
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M10–M20 | One source: Kennametal, its own catalog |
| Sandvik | GC2220 | CVD-coated carbide | Coated (process not printed) | M15–M30 (core M20) | One source: Sandvik Coromant, its own catalog |
| Seco | TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M20–M25 | One source: Seco Tools, its own catalog |
Why US7020 for austenitic stainless (304, 316)
US7020 for austenitic stainless (304, 316): rated M10–M30 (core M20) by Mitsubishi.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi rates US7020 (CVD-coated carbide) for M10–M30 (core M20): Stainless steel, continuous to light interrupted cutting.
One source: Mitsubishi Materials, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists US7020 at M10, M20. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)