Kennametal · CVD-coated carbide

KCM15 insert grade

KCM15 is Kennametal’s CVD-coated carbide grade (CVD, Multilayer MTCVD TiCN-Al2O3) for ISO P20–P25 and M10–M20, as Kennametal’s catalog prints it. Austenitic stainless, finishing to medium at higher speed; geometry and coating resist depth-of-cut notching and burrs.

One source: Kennametal, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO P and M.cutting edgecoating CVDsubstrate carbideISO groupPM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Kennametal prints

Type
CVD-coated carbide
Coating
CVD, Multilayer MTCVD TiCN-Al2O3
ISO P
P20–P25 · steel
ISO M
M10–M20 · stainless steel
Operations
turning
Twin
KCM15B (CVD, Multilayer MTCVD TiCN-Al2O3): Kennametal prints the same range and use

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

KCM15 equivalents by material

Steel · P

Read at P25, the centre of Kennametal’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC8250CVD-coated carbideCVD, TiCN + Al2O3 + TiNP10–P35

One source: ISCAR, its own catalog

MitsubishiMC6125CVD-coated carbideCVD, Accumulated TiCN-Al2O3-Ti compound, thickP10–P35 (core P20)

One source: Mitsubishi Materials, its own catalog

SandvikGC4325CVD-coated carbideCVDP10–P40 (core P25)

One source: Sandvik Coromant, its own catalog

Why KCM15 for steel

KCM15 for steel: rated P20–P25 by Kennametal.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.

    Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]

  3. So

    Kennametal rates KCM15 (CVD-coated carbide) for P20–P25: Austenitic stainless, finishing to medium at higher speed; geometry and coating resist depth-of-cut notching and burrs.

    One source: Kennametal, the maker of the grade , sources [5]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  4. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  5. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Stainless · M

Read at M15, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC6015CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M05–M25

One source: ISCAR, its own catalog

MitsubishiMC7015CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM05–M25 (core M15)

One source: Mitsubishi Materials, its own catalog

SandvikGC2015CVD-coated carbideCVDM05–M25 (core M15)

One source: Sandvik Coromant, its own catalog

SecoTM1501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M10–M20

One source: Seco Tools, its own catalog

Why KCM15 for austenitic stainless (304, 316)

KCM15 for austenitic stainless (304, 316): rated M10–M20 by Kennametal.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Kennametal rates KCM15 (CVD-coated carbide) for M10–M20: Austenitic stainless, finishing to medium at higher speed; geometry and coating resist depth-of-cut notching and burrs.

    One source: Kennametal, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists KCM15 at M10, M20. Kennametal’s own catalog is the authority for its grade.

It agrees with Kennametal’s catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)