ISCAR · CVD-coated carbide
IC9350 insert grade
IC9350 is ISCAR’s CVD-coated carbide grade (CVD, TiCN + alpha Al2O3 + TiN) for ISO P20–P45 and M15–M30, as ISCAR’s catalog prints it. Steel in interrupted and unstable cuts.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- CVD-coated carbide
- Coating
- CVD, TiCN + alpha Al2O3 + TiN
- Substrate
- Very tough, with a cobalt-enriched layer
- ISO P
- P20–P45 · steel
- ISO M
- M15–M30 · stainless steel
- Operations
- turning, milling
IC9350 equivalents by material
Steel · P
Read at P35, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Mitsubishi | MC6125 | CVD-coated carbide | CVD, Accumulated TiCN-Al2O3-Ti compound, thick | P10–P35 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why IC9350 for steel
IC9350 for steel: rated P20–P45 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
ISCAR rates IC9350 (CVD-coated carbide) for P20–P45: Steel in interrupted and unstable cuts.
One source: ISCAR, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC9350
Stainless · M
Read at M25, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M20–M30 | One source: Kennametal, its own catalog |
| Mitsubishi | MC7025 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2025 | CVD-coated carbide | CVD | M15–M35 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M20–M25 | One source: Seco Tools, its own catalog |
Why IC9350 for austenitic stainless (304, 316)
IC9350 for austenitic stainless (304, 316): rated M15–M30 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC9350 (CVD-coated carbide) for M15–M30: Steel in interrupted and unstable cuts.
One source: ISCAR, the maker of the grade , sources [4]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC9350 at P30, P40, M20, M30. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)