Mitsubishi · CVD-coated carbide

US905 insert grade

US905 is Mitsubishi’s CVD-coated carbide grade (CVD, TiCN-Al2O3-TiN, thin) for ISO S01–S10, as Mitsubishi’s catalog prints it. Heat resistant alloys, continuous and interrupted cutting.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO S.cutting edgecoating CVDsubstrate carbideISO groupS
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Mitsubishi prints

Type
CVD-coated carbide
Coating
CVD, TiCN-Al2O3-TiN, thin
Substrate
92.2 HRA
ISO S
S01–S10 (core S05) · superalloys and titanium
Operations
turning

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

US905 equivalents by material

ISO S (superalloys and titanium)

Read at S05, the centre of Mitsubishi’s S range (superalloys and titanium). Each grade is one its own maker rates for S05 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S05
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC804PVD-coated carbidePVD, AlTiN (SUMOTEC treated)S05–S15

One source: ISCAR, its own catalog

SandvikS05FCVD-coated carbideCVDS05–S15 (core S05)

One source: Sandvik Coromant, its own catalog

SecoTS0501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout S01–S05

One source: Seco Tools, its own catalog

Why US905 for heat-resistant superalloys (Inconel 718)

US905 for heat-resistant superalloys (Inconel 718): rated S01–S10 (core S05) by Mitsubishi.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Mitsubishi rates US905 (CVD-coated carbide) for S01–S10 (core S05): Heat resistant alloys, continuous and interrupted cutting.

    One source: Mitsubishi Materials, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a compilation across makers, lists US905 at S01. Mitsubishi Materials’ own catalog is the authority for its grade.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)