Sandvik · CVD-coated carbide
S05F insert grade
S05F is Sandvik’s CVD-coated carbide grade (CVD) for ISO S05–S15, as Sandvik’s catalog prints it. Superalloys: high-speed finishing, or long time in cut at lower speed, where notch wear does not dominate.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- CVD-coated carbide
- Coating
- CVD
- ISO S
- S05–S15 (core S05) · superalloys and titanium
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
S05F equivalents by material
ISO S (superalloys and titanium)
Read at S05, the centre of Sandvik’s S range (superalloys and titanium). Each grade is one its own maker rates for S05 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC804 | PVD-coated carbide | PVD, AlTiN (SUMOTEC treated) | S05–S15 | One source: ISCAR, its own catalog |
| Mitsubishi | US905 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | S01–S10 (core S05) | One source: Mitsubishi Materials, its own catalog |
| Seco | TS0501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about S01–S05 | One source: Seco Tools, its own catalog |
Why S05F for heat-resistant superalloys (Inconel 718)
S05F for heat-resistant superalloys (Inconel 718): rated S05–S15 (core S05) by Sandvik.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Sandvik rates S05F (CVD-coated carbide) for S05–S15 (core S05): Superalloys: high-speed finishing, or long time in cut at lower speed, where notch wear does not dominate.
One source: Sandvik Coromant, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists S05F at S01. Sandvik Coromant’s own catalog is the authority for its grade.
- The cross-reference lists S01; Sandvik Coromant gives S05–S15.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)