Seco · CVD-coated carbide
TS0501 insert grade
TS0501 is Seco’s CVD-coated carbide grade (CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer) for ISO S01–S05, as Seco’s catalog prints it. Semi-finishing to finishing of harder superalloys; sometimes hardened steel.
One source: Seco Tools, its own catalog
What Seco prints
- Type
- CVD-coated carbide
- Coating
- CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer
- Substrate
- Very hard super-micrograin
- ISO S
- about S01–S05 · superalloys and titanium
- Secondary
- ISO H (Seco names them in its text only)
- Operations
- turning
Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.
Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
TS0501 equivalents by material
ISO S (superalloys and titanium)
Read at S05, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S05 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC804 | PVD-coated carbide | PVD, AlTiN (SUMOTEC treated) | S05–S15 | One source: ISCAR, its own catalog |
| Mitsubishi | US905 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | S01–S10 (core S05) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | S05F | CVD-coated carbide | CVD | S05–S15 (core S05) | One source: Sandvik Coromant, its own catalog |
Why TS0501 for heat-resistant superalloys (Inconel 718)
TS0501 for heat-resistant superalloys (Inconel 718): rated about S01–S05 by Seco.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Seco rates TS0501 (CVD-coated carbide) for about S01–S05: Semi-finishing to finishing of harder superalloys; sometimes hardened steel.
One source: Seco Tools, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)