Mitsubishi · PVD-coated carbide
VP05RT insert grade
VP05RT is Mitsubishi’s PVD-coated carbide grade (PVD) for ISO S01–S20, as Mitsubishi’s catalog prints it. Heat resistant alloys, wear-resistant finishing.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- PVD-coated carbide
- Coating
- PVD
- ISO S
- S01–S20 (core S10) · superalloys and titanium
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
VP05RT equivalents by material
ISO S (superalloys and titanium)
Read at S10, the centre of Mitsubishi’s S range (superalloys and titanium). Each grade is one its own maker rates for S10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC804 | PVD-coated carbide | PVD, AlTiN (SUMOTEC treated) | S05–S15 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | TS2050 | PVD-coated carbide | PVD, Ti-Al-Si-N nanolaminate | about S05–S15 | One source: Seco Tools, its own catalog |
Why VP05RT for heat-resistant superalloys (Inconel 718)
VP05RT for heat-resistant superalloys (Inconel 718): rated S01–S20 (core S10) by Mitsubishi.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Mitsubishi rates VP05RT (PVD-coated carbide) for S01–S20 (core S10): Heat resistant alloys, wear-resistant finishing.
One source: Mitsubishi Materials, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists VP05RT at S01. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)