Sandvik · PVD-coated carbide

GC1125 insert grade

GC1125 is Sandvik’s PVD-coated carbide grade (PVD) for ISO M10–M30 and S20–S30, as Sandvik’s catalog prints it. Toughness-demanding stainless cuts; superalloys at low speed or light intermittent cuts.

One source: Sandvik Coromant, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO M and S.cutting edgecoating PVDsubstrate carbideISO groupMS
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Sandvik prints

Type
PVD-coated carbide
Coating
PVD
ISO M
M10–M30 (core M25) · stainless steel
ISO S
S20–S30 (core S25) · superalloys and titanium
Operations
turning

Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

GC1125 equivalents by material

Stainless · M

Read at M25, the centre of Sandvik’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC808PVD-coated carbidePVD, TiAlN/AlTiN + TiN (SUMOTEC)M20–M30

One source: ISCAR, its own catalog

KennametalKC5025PVD-coated carbidePVD, AlTiNM20–M30

One source: Kennametal, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDM10–M30 (core M20)

One source: Mitsubishi Materials, its own catalog

SecoCP500PVD-coated carbidePVD, (Ti,Al)N + TiNabout M10–M30

One source: Seco Tools, its own catalog

Why GC1125 for austenitic stainless (304, 316)

GC1125 for austenitic stainless (304, 316): rated M10–M30 (core M25) by Sandvik.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Sandvik rates GC1125 (PVD-coated carbide) for M10–M30 (core M25): Toughness-demanding stainless cuts; superalloys at low speed or light intermittent cuts.

    One source: Sandvik Coromant, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

Superalloys · S

Read at S25, the centre of Sandvik’s S range (superalloys and titanium). Each grade is one its own maker rates for S25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC328PVD-coated carbidePVD, TiCNS20–S30

One source: ISCAR, its own catalog

KennametalKC5025PVD-coated carbidePVD, AlTiNS20–S30

One source: Kennametal, its own catalog

MitsubishiMP9025PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS15–S35 (core S25)

One source: Mitsubishi Materials, its own catalog

Seco883micro-grain carbideUncoatedabout S10–S30

One source: Seco Tools, its own catalog

Why GC1125 for heat-resistant superalloys (Inconel 718)

GC1125 for heat-resistant superalloys (Inconel 718): rated S20–S30 (core S25) by Sandvik.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Sandvik rates GC1125 (PVD-coated carbide) for S20–S30 (core S25): Toughness-demanding stainless cuts; superalloys at low speed or light intermittent cuts.

    One source: Sandvik Coromant, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC1125 at P10, P20, P30, M20, M30, S20, S30. Sandvik Coromant’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)