ISCAR · PVD-coated carbide
IC328 insert grade
IC328 is ISCAR’s PVD-coated carbide grade (PVD, TiCN) for ISO P25–P40, M30–M40 and S20–S30, as ISCAR’s catalog prints it. Steel and stainless at low to medium speed, medium to high feed; interrupted and unstable cuts.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- PVD-coated carbide
- Coating
- PVD, TiCN
- Substrate
- Tough
- ISO P
- P25–P40 · steel
- ISO M
- M30–M40 · stainless steel
- ISO S
- S20–S30 · superalloys and titanium
- Operations
- turning, milling
IC328 equivalents by material
Steel · P
Read at P35, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | P20–P40 (core P30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why IC328 for steel
IC328 for steel: rated P25–P40 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC328 (PVD-coated carbide) for P25–P40: Steel and stainless at low to medium speed, medium to high feed; interrupted and unstable cuts.
One source: ISCAR, the maker of the grade , sources [3]
Stainless · M
Read at M35, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM35 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M30–M40 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2035 | PVD-coated carbide | PVD | M25–M40 (core M35) | One source: Sandvik Coromant, its own catalog |
| Seco | CP600 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M20–M40 | One source: Seco Tools, its own catalog |
Why IC328 for austenitic stainless (304, 316)
IC328 for austenitic stainless (304, 316): rated M30–M40 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC328 (PVD-coated carbide) for M30–M40: Steel and stainless at low to medium speed, medium to high feed; interrupted and unstable cuts.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC328
Superalloys · S
Read at S25, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | S20–S30 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9025 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S15–S35 (core S25) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1125 | PVD-coated carbide | PVD | S20–S30 (core S25) | One source: Sandvik Coromant, its own catalog |
| Seco | 883 | micro-grain carbide | Uncoated | about S10–S30 | One source: Seco Tools, its own catalog |
Why IC328 for heat-resistant superalloys (Inconel 718)
IC328 for heat-resistant superalloys (Inconel 718): rated S20–S30 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC328 (PVD-coated carbide) for S20–S30: Steel and stainless at low to medium speed, medium to high feed; interrupted and unstable cuts.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC328
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC328 at P20, P30, P40, M30, M40, S20. ISCAR’s own catalog is the authority for its grade.
- The cross-reference lists P20; ISCAR gives P25–P40.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)