Kennametal · PVD-coated carbide

KC5025 insert grade

KC5025 is Kennametal’s PVD-coated carbide grade (PVD, AlTiN) for ISO P20–P30, M20–M30, K20–K30, N20–N30 and S20–S30, as Kennametal’s catalog prints it. General purpose: steel, stainless, high-temperature alloys, titanium; low to medium speed, interruptions and high feeds.

One source: Kennametal, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P, M, K, N and S.cutting edgecoating PVDsubstrate carbideISO groupPMKNS
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Kennametal prints

Type
PVD-coated carbide
Coating
PVD, AlTiN
Substrate
Tough, ultra-fine-grain unalloyed carbide
ISO P
P20–P30 · steel
ISO M
M20–M30 · stainless steel
ISO K
K20–K30 · cast iron
ISO N
N20–N30 · non-ferrous
ISO S
S20–S30 · superalloys and titanium
Operations
turning

Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

KC5025 equivalents by material

Steel · P

Read at P25, the centre of Kennametal’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC250PVD-coated carbidePVD, TiCN + TiNP15–P35

One source: ISCAR, its own catalog

MitsubishiMS6015PVD-coated carbidePVDP10–P30 (core P20)

One source: Mitsubishi Materials, its own catalog

SandvikGC4325CVD-coated carbideCVDP10–P40 (core P25)

One source: Sandvik Coromant, its own catalog

Why KC5025 for steel

KC5025 for steel: rated P20–P30 by Kennametal.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Kennametal rates KC5025 (PVD-coated carbide) for P20–P30: General purpose: steel, stainless, high-temperature alloys, titanium; low to medium speed, interruptions and high feeds.

    One source: Kennametal, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Stainless · M

Read at M25, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC808PVD-coated carbidePVD, TiAlN/AlTiN + TiN (SUMOTEC)M20–M30

One source: ISCAR, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDM10–M30 (core M20)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDM10–M30 (core M25)

One source: Sandvik Coromant, its own catalog

SecoCP500PVD-coated carbidePVD, (Ti,Al)N + TiNabout M10–M30

One source: Seco Tools, its own catalog

Why KC5025 for austenitic stainless (304, 316)

KC5025 for austenitic stainless (304, 316): rated M20–M30 by Kennametal.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Kennametal rates KC5025 (PVD-coated carbide) for M20–M30: General purpose: steel, stainless, high-temperature alloys, titanium; low to medium speed, interruptions and high feeds.

    One source: Kennametal, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Cast iron · K

Read at K25, the centre of Kennametal’s K range (cast iron). Each grade is one its own maker rates for K25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC808PVD-coated carbidePVD, TiAlN/AlTiN + TiN (SUMOTEC)K20–K30

One source: ISCAR, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDK10–K30 (core K20)

One source: Mitsubishi Materials, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why KC5025 for gray cast iron

KC5025 for gray cast iron: rated K20–K30 by Kennametal.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Kennametal rates KC5025 (PVD-coated carbide) for K20–K30: General purpose: steel, stainless, high-temperature alloys, titanium; low to medium speed, interruptions and high feeds.

    One source: Kennametal, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Non-ferrous · N

Read at N25, the centre of Kennametal’s N range (non-ferrous). Each grade is one its own maker rates for N25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for N25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC228PVD-coated carbidePVD, AlTiN + TiNN20–N40

One source: ISCAR, its own catalog

SandvikH10uncoated carbideUncoatedN01–N25 (core N15)

One source: Sandvik Coromant, its own catalog

Why KC5025 for aluminum

KC5025 for aluminum: rated N20–N30 by Kennametal.

The reasoning, step by step
  1. The situation

    Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    It wants a sharp edge with low cutting force, one chips don’t weld to.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  3. So

    Kennametal rates KC5025 (PVD-coated carbide) for N20–N30: General purpose: steel, stainless, high-temperature alloys, titanium; low to medium speed, interruptions and high feeds.

    One source: Kennametal, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO N non-ferrous
  2. Mitsubishi Materials — Machining course: ISO group N, non-ferrous metals
  3. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

Superalloys · S

Read at S25, the centre of Kennametal’s S range (superalloys and titanium). Each grade is one its own maker rates for S25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC328PVD-coated carbidePVD, TiCNS20–S30

One source: ISCAR, its own catalog

MitsubishiMP9025PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS15–S35 (core S25)

One source: Mitsubishi Materials, its own catalog

SandvikGC1125PVD-coated carbidePVDS20–S30 (core S25)

One source: Sandvik Coromant, its own catalog

Seco883micro-grain carbideUncoatedabout S10–S30

One source: Seco Tools, its own catalog

Why KC5025 for heat-resistant superalloys (Inconel 718)

KC5025 for heat-resistant superalloys (Inconel 718): rated S20–S30 by Kennametal.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    Kennametal rates KC5025 (PVD-coated carbide) for S20–S30: General purpose: steel, stainless, high-temperature alloys, titanium; low to medium speed, interruptions and high feeds.

    One source: Kennametal, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists KC5025 at P20, S20. Kennametal’s own catalog is the authority for its grade.

It agrees with Kennametal’s catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)