Seco · micro-grain carbide

890 insert grade

890 is Seco’s micro-grain carbide grade (Uncoated) for ISO S10–S20, as Seco’s catalog prints it. Superalloys and titanium; other materials too.

One source: Seco Tools, its own catalog

The cutting edge of a micro-grain carbide insert in section: the micro-grain substrate, uncoated; rated for ISO S.cutting edgesubstrate micro-grainISO groupS
The edge in section; its ISO groups. Not to scale.

What Seco prints

Type
micro-grain carbide
Coating
Uncoated
Substrate
High-hardness micrograin
ISO S
about S10–S20 · superalloys and titanium
Secondary
ISO M, K, N, H (Seco names them in its text only)
Operations
turning

Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.

Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

890 equivalents by material

ISO S (superalloys and titanium)

Read at S15, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC1008PVD-coated carbidePVD, AlTiN + TiNS10–S20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedS10–S20

One source: Kennametal, its own catalog

MitsubishiMP9015PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS05–S25 (core S15)

One source: Mitsubishi Materials, its own catalog

SandvikGC1105PVD-coated carbidePVDS05–S20 (core S15)

One source: Sandvik Coromant, its own catalog

Why 890 for heat-resistant superalloys (Inconel 718)

890 for heat-resistant superalloys (Inconel 718): rated about S10–S20 by Seco.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Seco rates 890 (micro-grain carbide) for about S10–S20: Superalloys and titanium; other materials too.

    One source: Seco Tools, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists 890 at Z10, Z20. Seco Tools’ own catalog is the authority for its grade.

It agrees with Seco Tools’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)