Seco · uncoated carbide
HX insert grade
HX is Seco’s uncoated carbide grade (Uncoated) for ISO S10–S25, as Seco’s catalog prints it. Universal uncoated grade: cast iron, hardened steel and non-ferrous; main group superalloys.
One source: Seco Tools, its own catalog
What Seco prints
- Type
- uncoated carbide
- Coating
- Uncoated
- ISO S
- about S10–S25 · superalloys and titanium
- Secondary
- ISO M, K, N, H (Seco names them in its text only)
- Operations
- turning
Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.
Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
HX equivalents by material
ISO S (superalloys and titanium)
Read at S20, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC07 | uncoated carbide | Uncoated | S10–S30 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MT9015 | uncoated carbide | Uncoated | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | S10–S30 (core S15) | One source: Sandvik Coromant, its own catalog |
Why HX for heat-resistant superalloys (Inconel 718)
HX for heat-resistant superalloys (Inconel 718): rated about S10–S25 by Seco.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Seco rates HX (uncoated carbide) for about S10–S25: Universal uncoated grade: cast iron, hardened steel and non-ferrous; main group superalloys.
One source: Seco Tools, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists HX at M20, K20, N20, S10. Seco Tools’ own catalog is the authority for its grade.
It agrees with Seco Tools’ catalog.