ISCAR · uncoated carbide
IC07 insert grade
IC07 is ISCAR’s uncoated carbide grade (Uncoated) for ISO M10–M20, N05–N20 and S10–S30, as ISCAR’s catalog prints it. Aluminum and other non-ferrous at high speed.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- uncoated carbide
- Coating
- Uncoated
- Substrate
- Hard submicron grain
- ISO M
- M10–M20 · stainless steel
- ISO N
- N05–N20 · non-ferrous
- ISO S
- S10–S30 · superalloys and titanium
- Operations
- turning, milling
IC07 equivalents by material
Stainless · M
Read at M15, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | AP25N | cermet | PVD | M05–M25 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | TM1501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M10–M20 | One source: Seco Tools, its own catalog |
Why IC07 for austenitic stainless (304, 316)
IC07 for austenitic stainless (304, 316): rated M10–M20 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC07 (uncoated carbide) for M10–M20: Aluminum and other non-ferrous at high speed.
One source: ISCAR, the maker of the grade , sources [4]
Non-ferrous · N
Read at N15, the centre of ISCAR’s N range (non-ferrous). Each grade is one its own maker rates for N15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | N10–N20 | One source: Kennametal, its own catalog |
| Mitsubishi | HTi10 | uncoated carbide | Uncoated | N10–N20 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H10 | uncoated carbide | Uncoated | N01–N25 (core N15) | One source: Sandvik Coromant, its own catalog |
Why IC07 for aluminum
IC07 for aluminum: rated N05–N20 by ISCAR.
The reasoning, step by step
The situation
Aluminum is soft and sticky: it welds to the edge and spoils the finish. High-silicon alloys add hard particles that are abrasive.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
It wants a sharp edge with low cutting force, one chips don’t weld to.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC07 (uncoated carbide) for N05–N20: Aluminum and other non-ferrous at high speed.
One source: ISCAR, the maker of the grade , sources [3]
Superalloys · S
Read at S20, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MT9015 | uncoated carbide | Uncoated | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | S10–S30 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | HX | uncoated carbide | Uncoated | about S10–S25 | One source: Seco Tools, its own catalog |
Why IC07 for heat-resistant superalloys (Inconel 718)
IC07 for heat-resistant superalloys (Inconel 718): rated S10–S30 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC07 (uncoated carbide) for S10–S30: Aluminum and other non-ferrous at high speed.
One source: ISCAR, the maker of the grade , sources [4]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC07 at M10, M20, S10, S20. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)