Seco · PVD-coated carbide
TH1000 insert grade
TH1000 is Seco’s PVD-coated carbide grade (PVD, Ti-Al-Si-N nanolaminate) for ISO S01–S10 and H05–H15, as Seco’s catalog prints it. Partly hardened steel and hard-to-cut materials such as superalloys; tough enough for interrupted cuts.
One source: Seco Tools, its own catalog
What Seco prints
- Type
- PVD-coated carbide
- Coating
- PVD, Ti-Al-Si-N nanolaminate
- Substrate
- Very hard super-micrograin
- ISO S
- about S01–S10 · superalloys and titanium
- ISO H
- about H05–H15 · hardened steel
- Operations
- turning
Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.
Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
TH1000 equivalents by material
Superalloys · S
Read at S05, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S05 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC804 | PVD-coated carbide | PVD, AlTiN (SUMOTEC treated) | S05–S15 | One source: ISCAR, its own catalog |
| Mitsubishi | MP9005 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S01–S20 (core S10) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
Why TH1000 for heat-resistant superalloys (Inconel 718)
TH1000 for heat-resistant superalloys (Inconel 718): rated about S01–S10 by Seco.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Seco rates TH1000 (PVD-coated carbide) for about S01–S10: Partly hardened steel and hard-to-cut materials such as superalloys; tough enough for interrupted cuts.
One source: Seco Tools, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
Hardened · H
Read at H10, the centre of Seco’s H range (hardened steel). Each grade is one its own maker rates for H10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1007 | PVD-coated carbide | PVD, TiAlN | H05–H15 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | H10–H10 | One source: Kennametal, its own catalog |
Why TH1000 for hardened steel
TH1000 for hardened steel: rated about H05–H15 by Seco.
The reasoning, step by step
The situation
Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Seco rates TH1000 (PVD-coated carbide) for about H05–H15: Partly hardened steel and hard-to-cut materials such as superalloys; tough enough for interrupted cuts.
One source: Seco Tools, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists TH1000 at S01, S10. Seco Tools’ own catalog is the authority for its grade.
It agrees with Seco Tools’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)