IC1007 is ISCAR’s PVD-coated carbide grade (PVD, TiAlN) for ISO P10–P30, M05–M20, K20–K40, S05–S20 and H05–H15, as ISCAR’s catalog prints it. Heat resistant alloys, austenitic stainless and hard steel at low to medium speed.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- PVD-coated carbide
- Coating
- PVD, TiAlN
- Substrate
- Tough submicron
- ISO P
- P10–P30 · steel
- ISO M
- M05–M20 · stainless steel
- ISO K
- K20–K40 · cast iron
- ISO S
- S05–S20 · superalloys and titanium
- ISO H
- H05–H15 · hardened steel
- Operations
- turning, milling
IC1007 equivalents by material
Steel · P
Read at P20, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | P10–P20 | One source: Kennametal, its own catalog |
| Mitsubishi | MS6015 | PVD-coated carbide | PVD | P10–P30 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1525 | cermet | PVD | P05–P25 (core P15) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why IC1007 for steel
IC1007 for steel: rated P10–P30 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC1007 (PVD-coated carbide) for P10–P30: Heat resistant alloys, austenitic stainless and hard steel at low to medium speed.
One source: ISCAR, the maker of the grade , sources [3]
Stainless · M
Read at M15, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | VP10RT | PVD-coated carbide | PVD | M10–M30 (core M20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | CP500 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about M10–M30 | One source: Seco Tools, its own catalog |
Why IC1007 for austenitic stainless (304, 316)
IC1007 for austenitic stainless (304, 316): rated M05–M20 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC1007 (PVD-coated carbide) for M05–M20: Heat resistant alloys, austenitic stainless and hard steel at low to medium speed.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC1007
Cast iron · K
Read at K30, the centre of ISCAR’s K range (cast iron). Each grade is one its own maker rates for K30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | K20–K30 | One source: Kennametal, its own catalog |
| Mitsubishi | VP15TF | PVD-coated carbide | PVD | K20–K40 (core K30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why IC1007 for gray cast iron
IC1007 for gray cast iron: rated K20–K40 by ISCAR.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC1007 (PVD-coated carbide) for K20–K40: Heat resistant alloys, austenitic stainless and hard steel at low to medium speed.
One source: ISCAR, the maker of the grade , sources [3]
Superalloys · S
Read at S15, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | CP200 | PVD-coated carbide | PVD, (Ti,Al)N + TiN | about S10–S20 | One source: Seco Tools, its own catalog |
Why IC1007 for heat-resistant superalloys (Inconel 718)
IC1007 for heat-resistant superalloys (Inconel 718): rated S05–S20 by ISCAR.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
ISCAR rates IC1007 (PVD-coated carbide) for S05–S20: Heat resistant alloys, austenitic stainless and hard steel at low to medium speed.
One source: ISCAR, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC1007
Hardened · H
Read at H10, the centre of ISCAR’s H range (hardened steel). Each grade is one its own maker rates for H10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | H10–H10 | One source: Kennametal, its own catalog |
| Seco | TH1000 | PVD-coated carbide | PVD, Ti-Al-Si-N nanolaminate | about H05–H15 | One source: Seco Tools, its own catalog |
Why IC1007 for hardened steel
IC1007 for hardened steel: rated H05–H15 by ISCAR.
The reasoning, step by step
The situation
Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC1007 (PVD-coated carbide) for H05–H15: Heat resistant alloys, austenitic stainless and hard steel at low to medium speed.
One source: ISCAR, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC1007 at P20, M10, K20, K30. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)