Seco · PVD-coated carbide
TS2500 insert grade
TS2500 is Seco’s PVD-coated carbide grade (PVD, (Ti,Al)N + TiN) for ISO S10–S20, as Seco’s catalog prints it. Roughing superalloys and titanium; also stainless steel.
One source: Seco Tools, its own catalog
What Seco prints
- Type
- PVD-coated carbide
- Coating
- PVD, (Ti,Al)N + TiN
- Substrate
- Relatively hard micrograin
- ISO S
- about S10–S20 · superalloys and titanium
- Secondary
- ISO P, M, K (Seco names them in its text only)
- Operations
- turning
Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.
Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
TS2500 equivalents by material
ISO S (superalloys and titanium)
Read at S15, the centre of Seco’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC1008 | PVD-coated carbide | PVD, AlTiN + TiN | S10–S20 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | S10–S20 | One source: Kennametal, its own catalog |
| Mitsubishi | MP9015 | PVD-coated carbide | PVD, High-Al (Al,Ti)N, single layer | S05–S25 (core S15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1105 | PVD-coated carbide | PVD | S05–S20 (core S15) | One source: Sandvik Coromant, its own catalog |
Why TS2500 for heat-resistant superalloys (Inconel 718)
TS2500 for heat-resistant superalloys (Inconel 718): rated about S10–S20 by Seco.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.
Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]
So
Seco rates TS2500 (PVD-coated carbide) for about S10–S20: Roughing superalloys and titanium; also stainless steel.
One source: Seco Tools, the maker of the grade , sources [6]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists TS2500 at P20, M20, K20, S10, S20. Seco Tools’ own catalog is the authority for its grade.
It agrees with Seco Tools’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)