Pipe schedule chart
2" pipe schedule
NPS 2 (DN 50) pipe is 2.375" outside diameter in every schedule. Schedule 40 has a 0.154" wall and a 2.067" ID; Schedule 80 has a 0.218" wall and a 1.939" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
2.375"60.33 mm
NPS 2 · DN 50
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.0651.65 | 2.24557.02 | 1.612.39 | 0.4723.04 | 3.95825.54 | Checked against 4 published copies |
| Sch 10 · 10S | 0.1092.77 | 2.15754.79 | 2.643.93 | 0.7765.01 | 3.65423.58 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.1543.91 | 2.06752.50 | 3.665.44 | 1.0756.93 | 3.35621.65 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.2185.54 | 1.93949.25 | 5.037.48 | 1.4779.53 | 2.95319.05 | Checked against 4 published copies |
| Sch 160 | 0.3448.74 | 1.68742.85 | 7.4711.11 | 2.19514.16 | 2.23514.42 | Checked against 4 published copies |
| XXS | 0.43611.07 | 1.50338.18 | 9.0413.45 | 2.65617.13 | 1.77411.45 | Checked against 4 published copies |
Checked against 3 published copies
Notes for 2" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.154"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.218"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 2.375").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.