Pipe schedule chart

8" pipe schedule

NPS 8 (DN 200) pipe is 8.625" outside diameter in every schedule. Schedule 40 has a 0.322" wall and a 7.981" ID; Schedule 80 has a 0.500" wall and a 7.625" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 8.625" OD, in Schedule 40 and Schedule 80: the same OD, the wall setting the bore.OD 8.625"schedule 40ID 7.981"wall 0.322"schedule 80ID 7.625"wall 0.500"
8.625" OD pipe in Schedule 40 and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

8.625"219.08 mm

NPS 8 · DN 200

Checked against 5 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

8" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
5S0.1092.778.407213.549.9214.772.91618.8155.510358.13Checked against 4 published copies
Sch 10 · 10S0.1483.768.329211.5613.4119.963.94125.4354.485351.51Checked against 3 published copies
Sch 200.2506.358.125206.3822.3833.316.57842.4451.849334.51Checked against 4 published copies
Sch 300.2777.048.071205.0024.7236.797.26546.8751.162330.07Checked against 4 published copies
STD · Sch 40 · 40S0.3228.187.981202.7228.5842.538.39954.1950.027322.75Checked against 4 published copies
Sch 600.40610.317.813198.4535.6753.0910.48367.6347.943309.31Checked against 4 published copies
XS · Sch 80 · 80S0.50012.707.625193.6843.4364.6312.76382.3445.664294.60Checked against 4 published copies
Sch 1000.59415.097.437188.9051.0075.8914.98796.6943.440280.25Checked against 4 published copies
Sch 1200.71918.267.187182.5560.7790.4317.858115.2140.568261.73Checked against 4 published copies
Sch 1400.81220.627.001177.8367.82100.9319.931128.5938.496248.36Checked against 4 published copies
XXS0.87522.236.875174.6372.49107.8821.304137.4437.122239.50Checked against 4 published copies
Sch 1600.90623.016.813173.0574.76111.2521.970141.7436.456235.20Checked against 4 published copies

Checked against 3 published copies

Notes for 8" pipe

STD and XS, stainless, weight and what's not shown
  • STD and Sch 40 are the same wall here (0.322"). They part above NPS 10.
  • XS and Sch 80 are the same wall here (0.500"). They part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 8.625").

Sources

Sources8