Pipe schedule chart

20" pipe schedule

NPS 20 (DN 500) pipe is 20.000" outside diameter in every schedule. Schedule 40 has a 0.594" wall and a 18.812" ID; Schedule 80 has a 1.031" wall and a 17.938" ID. The schedule sets the wall: ID = OD − 2 × wall.

The pipe's cross section, 20" OD, in Schedule 40 and Schedule 80: the same OD, the wall setting the bore.OD 20"schedule 40ID 18.812"wall 0.594"schedule 80ID 17.938"wall 1.031"
20" OD pipe in Schedule 40 and Schedule 80. Each ring drawn to scale; the two to the same scale.

Outside diameter

20.000"508.00 mm

NPS 20 · DN 500

Checked against 4 published copies

Units

Every schedule

Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.

20" pipe wall, inside diameter, weight and areas by schedule
ScheduleWall (in)(mm)ID (in)(mm)Weight (lb/ft)(kg/m)Metal area (in²)(cm²)Flow area (in²)(cm²)Checked
5S0.1884.7819.624498.4539.8259.2511.70175.49302.4581,951.34Two published copies agree
10S0.2185.5419.564496.9346.1068.6013.54887.41300.6111,939.42Two published copies agree
Sch 100.2506.3519.500495.3052.7878.5515.512100.07298.6481,926.76Checked against 3 published copies
Sch 20 · STD · 40S0.3759.5319.250488.9578.67117.0823.120149.16291.0391,877.67Two published copies agree
Sch 30 · XS · 80S0.50012.7019.000482.60104.23155.1130.631197.62283.5291,829.21Two published copies agree
Sch 400.59415.0918.812477.82123.23183.3836.214233.64277.9461,793.19Two published copies agree
Sch 600.81220.6218.376466.75166.56247.8648.948315.79265.2111,711.04Two published copies agree
Sch 801.03126.1917.938455.63209.06311.1261.440396.39252.7191,630.44Checked against 3 published copies
Sch 1001.28132.5417.438442.93256.34381.4775.332486.01238.8271,540.82Checked against 3 published copies
Sch 1201.50038.1017.000431.80296.65441.4687.179562.45226.9801,464.38Checked against 3 published copies
Sch 1401.75044.4516.500419.10341.41508.08100.335647.32213.8251,379.51Checked against 3 published copies
Sch 1601.96950.0116.062407.97379.53564.80111.536719.59202.6231,307.24Checked against 3 published copies

Two published copies agree

  • Sch 40: Guanyu Tube (TubingChina) prints 5.94"; the other copies print 0.594".
  • Sch 60: Guanyu Tube (TubingChina) prints 8.12"; the other copies print 0.812".

Notes for 20" pipe

STD and XS, stainless, weight and what's not shown
  • STD (0.375") is not Sch 40 (0.594") at this size: they part above NPS 10.
  • XS (0.500") is not Sch 80 (1.031") at this size: they part above NPS 8.
  • Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
  • The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 20.000").

Sources

Sources7