Pipe schedule chart
6" pipe schedule
NPS 6 (DN 150) pipe is 6.625" outside diameter in every schedule. Schedule 40 has a 0.280" wall and a 6.065" ID; Schedule 80 has a 0.432" wall and a 5.761" ID. The schedule sets the wall: ID = OD − 2 × wall.
Outside diameter
6.625"168.28 mm
NPS 6 · DN 150
Checked against 5 published copies
Every schedule
Thinnest wall first. Schedules that share a wall share a row. Weight is plain-end carbon steel.
| Schedule | Wall (in)(mm) | ID (in)(mm) | Weight (lb/ft)(kg/m) | Metal area (in²)(cm²) | Flow area (in²)(cm²) | Checked |
|---|---|---|---|---|---|---|
| 5S | 0.1092.77 | 6.407162.74 | 7.5911.30 | 2.23114.40 | 32.240208.00 | Checked against 4 published copies |
| Sch 10 · 10S | 0.1343.40 | 6.357161.47 | 9.3013.84 | 2.73317.63 | 31.739204.77 | Checked against 3 published copies |
| STD · Sch 40 · 40S | 0.2807.11 | 6.065154.05 | 18.9928.26 | 5.58136.01 | 28.890186.39 | Checked against 4 published copies |
| XS · Sch 80 · 80S | 0.43210.97 | 5.761146.33 | 28.6042.56 | 8.40554.23 | 26.067168.17 | Checked against 4 published copies |
| Sch 120 | 0.56214.27 | 5.501139.73 | 36.4354.21 | 10.70569.06 | 23.767153.33 | Checked against 4 published copies |
| Sch 160 | 0.71918.26 | 5.187131.75 | 45.3967.55 | 13.34186.07 | 21.131136.33 | Checked against 4 published copies |
| XXS | 0.86421.95 | 4.897124.38 | 53.2179.18 | 15.637100.89 | 18.834121.51 | Checked against 4 published copies |
Checked against 3 published copies
Notes for 6" pipe
STD and XS, stainless, weight and what's not shown
- STD and Sch 40 are the same wall here (0.280"). They part above NPS 10.
- XS and Sch 80 are the same wall here (0.432"). They part above NPS 8.
- Schedules ending in S are stainless (ASME B36.19M). Same OD; the wall can differ from the carbon schedule of the same number.
- The weight is B36.10M's plain-end formula for carbon steel, 10.69 × (OD − wall) × wall lb/ft. For stainless or another metal, use the metal weight calculator (round tube, OD 6.625").
- Not shown: Sch 100 (only Project Materials prints it, 0.500").
Sources
Sources8
- ASME B36.10M, Welded and Seamless Wrought Steel Pipe (the authority for Sch 10–160, STD, XS, XXS)
- ASME B36.19M, Stainless Steel Pipe (the authority for 5S, 10S, 40S, 80S)
- Engineering ToolBox, ASME/ANSI B36.10/19 carbon, alloy and stainless steel pipe: dimensions (archived Oct 20, 2026)
- Engineers Edge, Standard pipe schedules and sizes chart (archived May 5, 2026)
- Project Materials, ASME B36.10 and B36.19 pipe sizes and schedules (inch, mm and lb/ft tables) (archived Jan 18, 2024)
- Guanyu Tube (TubingChina), ANSI standard steel pipe chart ASME B36.10 / B36.19 (archived Jun 30, 2025)
- Metal Supermarkets, Pipe schedule chart (Sch 40 and 80) (archived Apr 19, 2026)
- Project Materials, pipe weight: (OD − WT) × WT × 10.69 lb/ft for carbon steel (inch) (archived Jan 18, 2024)
Copies of B36.10M / B36.19M that print this size: Engineering ToolBox, Engineers Edge, Project Materials, Guanyu Tube (TubingChina), Metal Supermarkets.