ISO 286 · Fit · sliding
H7/g6 fit
H7/g6 at 25 mm: 0.007–0.041 mm clearance, a sliding fit. The hole is 25.000–25.021 mm and the shaft 24.980–24.993 mm. Fit guides agree it is for parts that slide and turn freely but locate accurately, such as shaft guides and sliding gears. The table gives it for every size to 500 mm.
H7/g6 by size range
Checked against 4 published copies
Every size to 500 mm
Hole and shaft deviations in µm. Fit: plus is clearance, minus is interference, from the loosest to the tightest pair. Each range is over the first size, up to and including the second.
| Size, mm | H7 µm | g6 µm | Loosest mm | Tightest mm | Loosest in | Tightest in |
|---|---|---|---|---|---|---|
| 0–3 | +10 / 0 | −2 / −8 | +0.018 | +0.002 | +0.00071 | +0.00008 |
| 3–6 | +12 / 0 | −4 / −12 | +0.024 | +0.004 | +0.00094 | +0.00016 |
| 6–10 | +15 / 0 | −5 / −14 | +0.029 | +0.005 | +0.00114 | +0.00020 |
| 10–18 | +18 / 0 | −6 / −17 | +0.035 | +0.006 | +0.00138 | +0.00024 |
| 18–30 | +21 / 0 | −7 / −20 | +0.041 | +0.007 | +0.00161 | +0.00028 |
| 30–50 | +25 / 0 | −9 / −25 | +0.050 | +0.009 | +0.00197 | +0.00035 |
| 50–80 | +30 / 0 | −10 / −29 | +0.059 | +0.010 | +0.00232 | +0.00039 |
| 80–120 | +35 / 0 | −12 / −34 | +0.069 | +0.012 | +0.00272 | +0.00047 |
| 120–180 | +40 / 0 | −14 / −39 | +0.079 | +0.014 | +0.00311 | +0.00055 |
| 180–250 | +46 / 0 | −15 / −44 | +0.090 | +0.015 | +0.00354 | +0.00059 |
| 250–315 | +52 / 0 | −17 / −49 | +0.101 | +0.017 | +0.00398 | +0.00067 |
| 315–400 | +57 / 0 | −18 / −54 | +0.111 | +0.018 | +0.00437 | +0.00071 |
| 400–500 | +63 / 0 | −20 / −60 | +0.123 | +0.020 | +0.00484 | +0.00079 |
Inches are the µm values ÷ 25,400. American inch fits (RC, LC, FN classes) are a different system.
What H7/g6 is for
For parts that slide and turn freely but locate accurately, such as shaft guides and sliding gears. 4 published fit guides agree on that.
The fit guides
- Wikipedia — Engineering fit (ISO fit tables) (archived Oct 20, 2026)
- AmesWeb — Preferred fits, ISO 286-1 and ANSI B4.2 (archived Sep 6, 2026)
- Fábrica do Projeto — Selection and application of ISO tolerances (archived Aug 15, 2025)
- TU Darmstadt IIM — Selection and calculation of fits (archived Nov 13, 2025)
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)