ISO 286 · Fit · locational interference
H7/p6 fit
H7/p6 at 25 mm: 0.001–0.035 mm interference, an interference fit. The hole is 25.000–25.021 mm and the shaft 25.022–25.035 mm. Fit guides agree it is for pressed-in hubs and bearing bushings. The table gives it for every size to 500 mm.
H7/p6 by size range
Checked against 4 published copies
Every size to 500 mm
Hole and shaft deviations in µm. Fit: plus is clearance, minus is interference, from the loosest to the tightest pair. Each range is over the first size, up to and including the second.
| Size, mm | H7 µm | p6 µm | Loosest mm | Tightest mm | Loosest in | Tightest in |
|---|---|---|---|---|---|---|
| 0–3 | +10 / 0 | +12 / +6 | +0.004 | −0.012 | +0.00016 | −0.00047 |
| 3–6 | +12 / 0 | +20 / +12 | 0 | −0.020 | 0 | −0.00079 |
| 6–10 | +15 / 0 | +24 / +15 | 0 | −0.024 | 0 | −0.00094 |
| 10–18 | +18 / 0 | +29 / +18 | 0 | −0.029 | 0 | −0.00114 |
| 18–30 | +21 / 0 | +35 / +22 | −0.001 | −0.035 | −0.00004 | −0.00138 |
| 30–50 | +25 / 0 | +42 / +26 | −0.001 | −0.042 | −0.00004 | −0.00165 |
| 50–80 | +30 / 0 | +51 / +32 | −0.002 | −0.051 | −0.00008 | −0.00201 |
| 80–120 | +35 / 0 | +59 / +37 | −0.002 | −0.059 | −0.00008 | −0.00232 |
| 120–180 | +40 / 0 | +68 / +43 | −0.003 | −0.068 | −0.00012 | −0.00268 |
| 180–250 | +46 / 0 | +79 / +50 | −0.004 | −0.079 | −0.00016 | −0.00311 |
| 250–315 | +52 / 0 | +88 / +56 | −0.004 | −0.088 | −0.00016 | −0.00346 |
| 315–400 | +57 / 0 | +98 / +62 | −0.005 | −0.098 | −0.00020 | −0.00386 |
| 400–500 | +63 / 0 | +108 / +68 | −0.005 | −0.108 | −0.00020 | −0.00425 |
Inches are the µm values ÷ 25,400. American inch fits (RC, LC, FN classes) are a different system.
What H7/p6 is for
For pressed-in hubs and bearing bushings. 2 published fit guides agree on that.
Sources
Sources4
ISO 286-1 and 286-2. Every limit on this page was checked against these published copies of the tables:
- Roymech — ISO tolerances for holes and shafts (ISO 286)
- CAD Forum — ISO 286-2 tolerances for holes and shafts (archived Sep 1, 2026)
- Mitsubishi Materials — Fit tolerance tables (shaft and hole) (archived Jun 3, 2024)
- Machining Doctor — Tolerance charts by deviation, holes and shafts (archived Jan 22, 2025)