ISCAR · CVD-coated carbide
IC6025 insert grade
IC6025 is ISCAR’s CVD-coated carbide grade (CVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)) for ISO M15–M35, as ISCAR’s catalog prints it. Stainless at moderate speed, medium to high feed; heavy, unstable and interrupted cuts.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- CVD-coated carbide
- Coating
- CVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)
- Substrate
- Very tough
- ISO M
- M15–M35 · stainless steel
- Operations
- turning, milling
IC6025 equivalents by material
ISO M (stainless steel)
Read at M25, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M20–M30 | One source: Kennametal, its own catalog |
| Mitsubishi | MC7025 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2025 | CVD-coated carbide | CVD | M15–M35 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M20–M25 | One source: Seco Tools, its own catalog |
Why IC6025 for austenitic stainless (304, 316)
IC6025 for austenitic stainless (304, 316): rated M15–M35 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC6025 (CVD-coated carbide) for M15–M35: Stainless at moderate speed, medium to high feed; heavy, unstable and interrupted cuts.
One source: ISCAR, the maker of the grade , sources [4]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC6025 at M30, M40. ISCAR’s own catalog is the authority for its grade.
- The cross-reference lists M40; ISCAR gives M15–M35.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)