Sandvik · CVD-coated carbide
GC2025 insert grade
GC2025 is Sandvik’s CVD-coated carbide grade (CVD) for ISO M15–M35, as Sandvik’s catalog prints it. Stainless steel, semi-finishing to roughing; handles interrupted cuts.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- CVD-coated carbide
- Coating
- CVD
- ISO M
- M15–M35 (core M25) · stainless steel
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
GC2025 equivalents by material
ISO M (stainless steel)
Read at M25, the centre of Sandvik’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC4050 | CVD-coated carbide | CVD, TiCN + Al2O3 + TiN | M20–M30 | One source: ISCAR, its own catalog |
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M20–M30 | One source: Kennametal, its own catalog |
| Mitsubishi | MC7025 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Seco | TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M20–M25 | One source: Seco Tools, its own catalog |
Why GC2025 for austenitic stainless (304, 316)
GC2025 for austenitic stainless (304, 316): rated M15–M35 (core M25) by Sandvik.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Sandvik rates GC2025 (CVD-coated carbide) for M15–M35 (core M25): Stainless steel, semi-finishing to roughing; handles interrupted cuts.
One source: Sandvik Coromant, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC2025 at M30, M40. Sandvik Coromant’s own catalog is the authority for its grade.
- The cross-reference lists M40; Sandvik Coromant gives M15–M35.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)