Kennametal · CVD-coated carbide
KCM25 insert grade
KCM25 is Kennametal’s CVD-coated carbide grade (CVD, Multilayer MTCVD TiCN-Al2O3) for ISO P35–P45 and M20–M30, as Kennametal’s catalog prints it. General-purpose austenitic stainless at moderate speeds and feeds; resists built-up edge.
One source: Kennametal, its own catalog
What Kennametal prints
- Type
- CVD-coated carbide
- Coating
- CVD, Multilayer MTCVD TiCN-Al2O3
- Substrate
- Tough, cobalt-enriched carbide
- ISO P
- P35–P45 · steel
- ISO M
- M20–M30 · stainless steel
- Operations
- turning
- Twin
- KCM25B (CVD, Multilayer MTCVD TiCN-Al2O3-TiOCN): Kennametal prints the same range and use
Source: Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
KCM25 equivalents by material
Steel · P
Read at P40, the centre of Kennametal’s P range (steel). Each grade is one its own maker rates for P40 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC635 | CVD-coated carbide | CVD, TiN + TiC + TiN | P30–P50 | One source: ISCAR, its own catalog |
| Mitsubishi | UTi20T | uncoated carbide | Uncoated | P25–P40 (core P35) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why KCM25 for steel
KCM25 for steel: rated P35–P45 by Kennametal.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
Kennametal rates KCM25 (CVD-coated carbide) for P35–P45: General-purpose austenitic stainless at moderate speeds and feeds; resists built-up edge.
One source: Kennametal, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
Stainless · M
Read at M25, the centre of Kennametal’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC4050 | CVD-coated carbide | CVD, TiCN + Al2O3 + TiN | M20–M30 | One source: ISCAR, its own catalog |
| Mitsubishi | MC7025 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2025 | CVD-coated carbide | CVD | M15–M35 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M20–M25 | One source: Seco Tools, its own catalog |
Why KCM25 for austenitic stainless (304, 316)
KCM25 for austenitic stainless (304, 316): rated M20–M30 by Kennametal.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Kennametal rates KCM25 (CVD-coated carbide) for M20–M30: General-purpose austenitic stainless at moderate speeds and feeds; resists built-up edge.
One source: Kennametal, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Kennametal — Master Catalog 2018, Vol. 1 Turning Tools (inch), grades and grade descriptions (pp. B22–B29) (archived Jun 4, 2023)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists KCM25 at M30. Kennametal’s own catalog is the authority for its grade.
It agrees with Kennametal’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)