Mitsubishi · CVD-coated carbide

MC7025 insert grade

MC7025 is Mitsubishi’s CVD-coated carbide grade (CVD, TiCN-Al2O3-TiN, thin) for ISO M20–M40, as Mitsubishi’s catalog prints it. Stainless steel, general (medium) cutting.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO M.cutting edgecoating CVDsubstrate carbideISO groupM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Mitsubishi prints

Type
CVD-coated carbide
Coating
CVD, TiCN-Al2O3-TiN, thin
Substrate
89.4 HRA
ISO M
M20–M40 (core M30) · stainless steel
Operations
turning

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

Mitsubishi’s first choice

  • Mitsubishi names MC7025 its first choice for stainless steel under 200 HB (e.g. 304, 316), general conditions: finishing, medium and roughing.

One source: Mitsubishi Materials, its own catalog

Open the insert picker

MC7025 equivalents by material

ISO M (stainless steel)

Read at M30, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M30
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC635CVD-coated carbideCVD, TiN + TiC + TiNM20–M40

One source: ISCAR, its own catalog

KennametalKCM25CVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3M20–M30

One source: Kennametal, its own catalog

SandvikGC2025CVD-coated carbideCVDM15–M35 (core M25)

One source: Sandvik Coromant, its own catalog

SecoTM3501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M25–M35

One source: Seco Tools, its own catalog

Why MC7025 for austenitic stainless (304, 316)

MC7025 for austenitic stainless (304, 316): rated M20–M40 (core M30) by Mitsubishi.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Mitsubishi rates MC7025 (CVD-coated carbide) for M20–M40 (core M30): Stainless steel, general (medium) cutting.

    One source: Mitsubishi Materials, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a compilation across makers, lists MC7025 at M20, M30. Mitsubishi Materials’ own catalog is the authority for its grade.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)