ISCAR · CVD-coated carbide
IC8250 insert grade
IC8250 is ISCAR’s CVD-coated carbide grade (CVD, TiCN + Al2O3 + TiN) for ISO P10–P35 and M05–M20, as ISCAR’s catalog prints it. General steel machining over a wide range of conditions.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- CVD-coated carbide
- Coating
- CVD, TiCN + Al2O3 + TiN
- Substrate
- Tough, with a cobalt-enriched layer
- ISO P
- P10–P35 · steel
- ISO M
- M05–M20 · stainless steel
- Operations
- turning, milling
- Twin
- IC9250 (CVD, TiCN + alpha Al2O3 + TiN): ISCAR prints the same range and use
IC8250 equivalents by material
Steel · P
Read at P25, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P20–P25 | One source: Kennametal, its own catalog |
| Mitsubishi | MC6125 | CVD-coated carbide | CVD, Accumulated TiCN-Al2O3-Ti compound, thick | P10–P35 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4325 | CVD-coated carbide | CVD | P10–P40 (core P25) | One source: Sandvik Coromant, its own catalog |
Why IC8250 for steel
IC8250 for steel: rated P10–P35 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
ISCAR rates IC8250 (CVD-coated carbide) for P10–P35: General steel machining over a wide range of conditions.
One source: ISCAR, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC8250
Stainless · M
Read at M15, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | MC7015 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M05–M25 (core M15) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2015 | CVD-coated carbide | CVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | TM1501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M10–M20 | One source: Seco Tools, its own catalog |
Why IC8250 for austenitic stainless (304, 316)
IC8250 for austenitic stainless (304, 316): rated M05–M20 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC8250 (CVD-coated carbide) for M05–M20: General steel machining over a wide range of conditions.
One source: ISCAR, the maker of the grade , sources [4]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC8250 at P10, P20, M10. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)