Seco · cermet
TP1030 insert grade
TP1030 is Seco’s cermet grade (PVD, Ti-Al-Si-N nanolaminate) for ISO P10–P20, as Seco’s catalog prints it. Coated cermet for high surface finish, mainly in steel and stainless.
One source: Seco Tools, its own catalog
What Seco prints
- Type
- cermet
- Coating
- PVD, Ti-Al-Si-N nanolaminate
- ISO P
- about P10–P20 · steel
- Secondary
- ISO M (Seco names them in its text only)
- Operations
- turning
Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.
Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)
TP1030 equivalents by material
ISO P (steel)
Read at P15, the centre of Seco’s P range (steel). Each grade is one its own maker rates for P15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC30N | cermet | Uncoated | P10–P30 | One source: ISCAR, its own catalog |
| Kennametal | KC5010 | PVD-coated carbide | PVD, AlTiN | P10–P20 | One source: Kennametal, its own catalog |
| Mitsubishi | AP25N | cermet | PVD | P05–P25 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1525 | cermet | PVD | P05–P25 (core P15) | One source: Sandvik Coromant, its own catalog |
Why TP1030 for steel
TP1030 for steel: rated about P10–P20 by Seco.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
Seco rates TP1030 (cermet) for about P10–P20: Coated cermet for high surface finish, mainly in steel and stainless.
One source: Seco Tools, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists TP1030 at P10, P20, M10. Seco Tools’ own catalog is the authority for its grade.
It agrees with Seco Tools’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)