Mitsubishi · CVD-coated carbide
MC6125 insert grade
MC6125 is Mitsubishi’s CVD-coated carbide grade (CVD, Accumulated TiCN-Al2O3-Ti compound, thick) for ISO P10–P35, as Mitsubishi’s catalog prints it. Steel, continuous to interrupted cutting; the general-purpose grade of the MC6100 series.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- CVD-coated carbide
- Coating
- CVD, Accumulated TiCN-Al2O3-Ti compound, thick
- Substrate
- 90.0 HRA
- ISO P
- P10–P35 (core P20) · steel
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names MC6125 its first choice for carbon and alloy steel, 180–280 HB (e.g. 1045, 4140), general conditions: medium and roughing.
- Mitsubishi names MC6125 its first choice for carbon and alloy steel, 180–280 HB (e.g. 1045, 4140), unstable conditions: medium.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerMC6125 equivalents by material
ISO P (steel)
Read at P20, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC8250 | CVD-coated carbide | CVD, TiCN + Al2O3 + TiN | P10–P35 | One source: ISCAR, its own catalog |
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P20–P25 | One source: Kennametal, its own catalog |
| Sandvik | GC4315 | CVD-coated carbide | CVD | P01–P30 (core P15) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why MC6125 for steel
MC6125 for steel: rated P10–P35 (core P20) by Mitsubishi.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
Mitsubishi rates MC6125 (CVD-coated carbide) for P10–P35 (core P20): Steel, continuous to interrupted cutting; the general-purpose grade of the MC6100 series.
One source: Mitsubishi Materials, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)