Mitsubishi · CVD-coated carbide
MC7015 insert grade
MC7015 is Mitsubishi’s CVD-coated carbide grade (CVD, TiCN-Al2O3-TiN, thin) for ISO M05–M25, as Mitsubishi’s catalog prints it. Stainless steel, continuous cutting at high speed.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- CVD-coated carbide
- Coating
- CVD, TiCN-Al2O3-TiN, thin
- Substrate
- 90.7 HRA
- ISO M
- M05–M25 (core M15) · stainless steel
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
Mitsubishi’s first choice
- Mitsubishi names MC7015 its first choice for stainless steel under 200 HB (e.g. 304, 316), stable conditions: finishing, medium and roughing.
One source: Mitsubishi Materials, its own catalog
Open the insert pickerMC7015 equivalents by material
ISO M (stainless steel)
Read at M15, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC6015 | CVD-coated carbide | CVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated) | M05–M25 | One source: ISCAR, its own catalog |
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M10–M20 | One source: Kennametal, its own catalog |
| Sandvik | GC2015 | CVD-coated carbide | CVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | TM1501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M10–M20 | One source: Seco Tools, its own catalog |
Why MC7015 for austenitic stainless (304, 316)
MC7015 for austenitic stainless (304, 316): rated M05–M25 (core M15) by Mitsubishi.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi rates MC7015 (CVD-coated carbide) for M05–M25 (core M15): Stainless steel, continuous cutting at high speed.
One source: Mitsubishi Materials, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO M stainless
- Mitsubishi Materials — Machining course: ISO group M, stainless steel
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists MC7015 at M10, M20. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)