Seco · CVD-coated carbide

TM1501 insert grade

TM1501 is Seco’s CVD-coated carbide grade (CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer) for ISO M10–M20, as Seco’s catalog prints it. Continuous cuts in stainless steel; mixed steel and stainless work.

One source: Seco Tools, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO M.cutting edgecoating CVDsubstrate carbideISO groupM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Seco prints

Type
CVD-coated carbide
Coating
CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer
ISO M
about M10–M20 · stainless steel
Secondary
ISO P (Seco names them in its text only)
Operations
turning

Seco draws its ranges as ovals on an ISO chart with no numbers; these are read off the chart, good to about one step.

Source: Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)

TM1501 equivalents by material

ISO M (stainless steel)

Read at M15, the centre of Seco’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC6015CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M05–M25

One source: ISCAR, its own catalog

KennametalKCM15CVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3M10–M20

One source: Kennametal, its own catalog

MitsubishiMC7015CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM05–M25 (core M15)

One source: Mitsubishi Materials, its own catalog

SandvikGC2015CVD-coated carbideCVDM05–M25 (core M15)

One source: Sandvik Coromant, its own catalog

Why TM1501 for austenitic stainless (304, 316)

TM1501 for austenitic stainless (304, 316): rated about M10–M20 by Seco.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Seco rates TM1501 (CVD-coated carbide) for about M10–M20: Continuous cuts in stainless steel; mixed steel and stainless work.

    One source: Seco Tools, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Seco Tools — Turning catalogue 2026.2: insert grades (p. 68) and grade descriptions (pp. 119–122) (archived Nov 16, 2026)