GC2015 insert grade

GC2015 is Sandvik’s CVD-coated carbide grade (CVD) for ISO M05–M25, as Sandvik’s catalog prints it. Stainless steel, finishing and light roughing; continuous cuts at moderate to high speed.

One source: Sandvik Coromant, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO M.cutting edgecoating CVDsubstrate carbideISO groupM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Sandvik prints

Type
CVD-coated carbide
Coating
CVD
ISO M
M05–M25 (core M15) · stainless steel
Operations
turning

Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

GC2015 equivalents by material

ISO M (stainless steel)

Read at M15, the centre of Sandvik’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC6015CVD-coated carbideCVD, TiCN + Al2O3 + TiN (MTCVD, SUMOTEC treated)M05–M25

One source: ISCAR, its own catalog

KennametalKCM15CVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3M10–M20

One source: Kennametal, its own catalog

MitsubishiMC7015CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM05–M25 (core M15)

One source: Mitsubishi Materials, its own catalog

SecoTM1501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M10–M20

One source: Seco Tools, its own catalog

Why GC2015 for austenitic stainless (304, 316)

GC2015 for austenitic stainless (304, 316): rated M05–M25 (core M15) by Sandvik.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Sandvik rates GC2015 (CVD-coated carbide) for M05–M25 (core M15): Stainless steel, finishing and light roughing; continuous cuts at moderate to high speed.

    One source: Sandvik Coromant, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC2015 at M10, M20. Sandvik Coromant’s own catalog is the authority for its grade.

It agrees with Sandvik Coromant’s catalog.