ISCAR · CVD-coated carbide

IC635 insert grade

IC635 is ISCAR’s CVD-coated carbide grade (CVD, TiN + TiC + TiN) for ISO P30–P50 and M20–M40, as ISCAR’s catalog prints it. Low speed, high feed, unfavorable conditions.

One source: ISCAR, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO P and M.cutting edgecoating CVDsubstrate carbideISO groupPM
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What ISCAR prints

Type
CVD-coated carbide
Coating
CVD, TiN + TiC + TiN
ISO P
P30–P50 · steel
ISO M
M20–M40 · stainless steel
Operations
turning, milling

Source: ISCAR — eCatalog grade data: IC635

IC635 equivalents by material

Steel · P

Read at P40, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P40 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P40
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKCM25CVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3P35–P45

One source: Kennametal, its own catalog

MitsubishiUTi20Tuncoated carbideUncoatedP25–P40 (core P35)

One source: Mitsubishi Materials, its own catalog

SandvikGC4335CVD-coated carbideCVDP25–P45 (core P35)

One source: Sandvik Coromant, its own catalog

Why IC635 for steel

IC635 for steel: rated P30–P50 by ISCAR.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.

    Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]

  3. So

    ISCAR rates IC635 (CVD-coated carbide) for P30–P50: Low speed, high feed, unfavorable conditions.

    One source: ISCAR, the maker of the grade , sources [5]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  4. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  5. ISCAR — eCatalog grade data: IC635

Stainless · M

Read at M30, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M30
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKCM25CVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3M20–M30

One source: Kennametal, its own catalog

MitsubishiMC7025CVD-coated carbideCVD, TiCN-Al2O3-TiN, thinM20–M40 (core M30)

One source: Mitsubishi Materials, its own catalog

SandvikGC2025CVD-coated carbideCVDM15–M35 (core M25)

One source: Sandvik Coromant, its own catalog

SecoTM3501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M25–M35

One source: Seco Tools, its own catalog

Why IC635 for austenitic stainless (304, 316)

IC635 for austenitic stainless (304, 316): rated M20–M40 by ISCAR.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    ISCAR rates IC635 (CVD-coated carbide) for M20–M40: Low speed, high feed, unfavorable conditions.

    One source: ISCAR, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. ISCAR — eCatalog grade data: IC635

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC635 at M40. ISCAR’s own catalog is the authority for its grade.

It agrees with ISCAR’s catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)