Mitsubishi · PVD-coated carbide

MS6015 insert grade

MS6015 is Mitsubishi’s PVD-coated carbide grade (PVD) for ISO P10–P30, as Mitsubishi’s catalog prints it. Steel, for high-precision and small-part machining.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P.cutting edgecoating PVDsubstrate carbideISO groupP
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Mitsubishi prints

Type
PVD-coated carbide
Coating
PVD
ISO P
P10–P30 (core P20) · steel
Operations
turning

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

MS6015 equivalents by material

ISO P (steel)

Read at P20, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P20
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC1007PVD-coated carbidePVD, TiAlNP10–P30

One source: ISCAR, its own catalog

KennametalKC5010PVD-coated carbidePVD, AlTiNP10–P20

One source: Kennametal, its own catalog

SandvikGC1525cermetPVDP05–P25 (core P15)

One source: Sandvik Coromant, its own catalog

SecoTP1030cermetPVD, Ti-Al-Si-N nanolaminateabout P10–P20

One source: Seco Tools, its own catalog

Why MS6015 for steel

MS6015 for steel: rated P10–P30 (core P20) by Mitsubishi.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Mitsubishi rates MS6015 (PVD-coated carbide) for P10–P30 (core P20): Steel, for high-precision and small-part machining.

    One source: Mitsubishi Materials, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a compilation across makers, lists MS6015 at P10, P20, M10. Mitsubishi Materials’ own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)