Sandvik · cermet

GC1525 insert grade

GC1525 is Sandvik’s cermet grade (PVD) for ISO P05–P25, as Sandvik’s catalog prints it. PVD-coated cermet for finishing and semi-finishing low-carbon and low-alloy steel at medium to high speed.

One source: Sandvik Coromant, its own catalog

The cutting edge of a cermet insert in section: the cermet substrate, uncoated; rated for ISO P.cutting edgesubstrate cermetISO groupP
The edge in section; its ISO groups. Not to scale.

What Sandvik prints

Type
cermet
Coating
PVD
ISO P
P05–P25 (core P15) · steel
Operations
turning

Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

GC1525 equivalents by material

ISO P (steel)

Read at P15, the centre of Sandvik’s P range (steel). Each grade is one its own maker rates for P15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC30NcermetUncoatedP10–P30

One source: ISCAR, its own catalog

KennametalKC5010PVD-coated carbidePVD, AlTiNP10–P20

One source: Kennametal, its own catalog

MitsubishiAP25NcermetPVDP05–P25

One source: Mitsubishi Materials, its own catalog

SecoTP1030cermetPVD, Ti-Al-Si-N nanolaminateabout P10–P20

One source: Seco Tools, its own catalog

Why GC1525 for steel

GC1525 for steel: rated P05–P25 (core P15) by Sandvik.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Sandvik rates GC1525 (cermet) for P05–P25 (core P15): PVD-coated cermet for finishing and semi-finishing low-carbon and low-alloy steel at medium to high speed.

    One source: Sandvik Coromant, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC1525 at P10, P20, M10. Sandvik Coromant’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)