Mitsubishi · uncoated carbide
MT9005 insert grade
MT9005 is Mitsubishi’s uncoated carbide grade (Uncoated) for ISO S01–S20, as Mitsubishi’s catalog prints it. Titanium alloys and heat resistant alloys.
One source: Mitsubishi Materials, its own catalog
What Mitsubishi prints
- Type
- uncoated carbide
- Coating
- Uncoated
- Substrate
- WC-Co
- ISO S
- S01–S20 (core S10) · superalloys and titanium
- Operations
- turning
Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
MT9005 equivalents by material
ISO S (superalloys and titanium)
Read at S10, the centre of Mitsubishi’s S range (superalloys and titanium). Each grade is one its own maker rates for S10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC20 | uncoated carbide | Uncoated | S05–S20 | One source: ISCAR, its own catalog |
| Kennametal | K313 | uncoated carbide | Uncoated | S10–S20 | One source: Kennametal, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | S10–S30 (core S15) | One source: Sandvik Coromant, its own catalog |
| Seco | HX | uncoated carbide | Uncoated | about S10–S25 | One source: Seco Tools, its own catalog |
Why MT9005 for heat-resistant superalloys (Inconel 718)
MT9005 for heat-resistant superalloys (Inconel 718): rated S01–S20 (core S10) by Mitsubishi.
The reasoning, step by step
The situation
Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
Mitsubishi rates MT9005 (uncoated carbide) for S01–S20 (core S10): Titanium alloys and heat resistant alloys.
One source: Mitsubishi Materials, the maker of the grade , sources [4]
- Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
- Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
- NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
- Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a compilation across makers, lists MT9005 at S01, S10. Mitsubishi Materials’ own catalog is the authority for its grade.
It agrees with Mitsubishi Materials’ catalog.