Mitsubishi · micro-grain carbide

TF15 insert grade

TF15 is Mitsubishi’s micro-grain carbide grade (Uncoated) for ISO K20–K20, as Mitsubishi’s catalog prints it. Micro-grain grade for turning steel and cast iron.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a micro-grain carbide insert in section: the micro-grain substrate, uncoated; rated for ISO K.cutting edgesubstrate micro-grainISO groupK
The edge in section; its ISO groups. Not to scale.

What Mitsubishi prints

Type
micro-grain carbide
Coating
Uncoated
Substrate
Micro-grain, 91.0 HRA, TRS 4.0 GPa
ISO K
K20–K20 · cast iron
Operations
turning

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

TF15 equivalents by material

ISO K (cast iron)

Read at K20, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K20
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC807PVD-coated carbidePVD, TiAlN + TiN (SUMOTEC treated)K10–K30

One source: ISCAR, its own catalog

KennametalKC5025PVD-coated carbidePVD, AlTiNK20–K30

One source: Kennametal, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why TF15 for gray cast iron

TF15 for gray cast iron: rated K20–K20 by Mitsubishi.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Mitsubishi rates TF15 (micro-grain carbide) for K20–K20: Micro-grain grade for turning steel and cast iron.

    One source: Mitsubishi Materials, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a compilation across makers, lists TF15 at Z20. Mitsubishi Materials’ own catalog is the authority for its grade.

It agrees with Mitsubishi Materials’ catalog.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)