ISCAR · PVD-coated carbide

IC807 insert grade

IC807 is ISCAR’s PVD-coated carbide grade (PVD, TiAlN + TiN (SUMOTEC treated)) for ISO P10–P30, M05–M20, K10–K30, S05–S20 and H05–H15, as ISCAR’s catalog prints it. Steel, austenitic stainless, high-temperature alloys and hard steel at moderate to fairly high speed, stable conditions.

One source: ISCAR, its own catalog

The cutting edge of a PVD-coated carbide insert in section: the carbide substrate under its PVD coating; rated for ISO P, M, K, S and H.cutting edgecoating PVDsubstrate carbideISO groupPMKSH
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What ISCAR prints

Type
PVD-coated carbide
Coating
PVD, TiAlN + TiN (SUMOTEC treated)
Substrate
Hard submicron
ISO P
P10–P30 · steel
ISO M
M05–M20 · stainless steel
ISO K
K10–K30 · cast iron
ISO S
S05–S20 · superalloys and titanium
ISO H
H05–H15 · hardened steel
Operations
turning, milling

Source: ISCAR — eCatalog grade data: IC807

IC807 equivalents by material

Steel · P

Read at P20, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P20
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5010PVD-coated carbidePVD, AlTiNP10–P20

One source: Kennametal, its own catalog

MitsubishiMS6015PVD-coated carbidePVDP10–P30 (core P20)

One source: Mitsubishi Materials, its own catalog

SandvikGC1525cermetPVDP05–P25 (core P15)

One source: Sandvik Coromant, its own catalog

SecoTP1030cermetPVD, Ti-Al-Si-N nanolaminateabout P10–P20

One source: Seco Tools, its own catalog

Why IC807 for steel

IC807 for steel: rated P10–P30 by ISCAR.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC807 (PVD-coated carbide) for P10–P30: Steel, austenitic stainless, high-temperature alloys and hard steel at moderate to fairly high speed, stable conditions.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. ISCAR — eCatalog grade data: IC807

Stainless · M

Read at M15, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M15
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5010PVD-coated carbidePVD, AlTiNM10–M20

One source: Kennametal, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDM10–M30 (core M20)

One source: Mitsubishi Materials, its own catalog

SandvikGC1115PVD-coated carbidePVDM05–M25 (core M15)

One source: Sandvik Coromant, its own catalog

SecoCP500PVD-coated carbidePVD, (Ti,Al)N + TiNabout M10–M30

One source: Seco Tools, its own catalog

Why IC807 for austenitic stainless (304, 316)

IC807 for austenitic stainless (304, 316): rated M05–M20 by ISCAR.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC807 (PVD-coated carbide) for M05–M20: Steel, austenitic stainless, high-temperature alloys and hard steel at moderate to fairly high speed, stable conditions.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC807

Cast iron · K

Read at K20, the centre of ISCAR’s K range (cast iron). Each grade is one its own maker rates for K20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K20
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5025PVD-coated carbidePVD, AlTiNK20–K30

One source: Kennametal, its own catalog

MitsubishiVP10RTPVD-coated carbidePVDK10–K30 (core K20)

One source: Mitsubishi Materials, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why IC807 for gray cast iron

IC807 for gray cast iron: rated K10–K30 by ISCAR.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC807 (PVD-coated carbide) for K10–K30: Steel, austenitic stainless, high-temperature alloys and hard steel at moderate to fairly high speed, stable conditions.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. ISCAR — eCatalog grade data: IC807

Superalloys · S

Read at S15, the centre of ISCAR’s S range (superalloys and titanium). Each grade is one its own maker rates for S15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for S15
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5010PVD-coated carbidePVD, AlTiNS10–S20

One source: Kennametal, its own catalog

MitsubishiMP9015PVD-coated carbidePVD, High-Al (Al,Ti)N, single layerS05–S25 (core S15)

One source: Mitsubishi Materials, its own catalog

SandvikGC1105PVD-coated carbidePVDS05–S20 (core S15)

One source: Sandvik Coromant, its own catalog

SecoCP200PVD-coated carbidePVD, (Ti,Al)N + TiNabout S10–S20

One source: Seco Tools, its own catalog

Why IC807 for heat-resistant superalloys (Inconel 718)

IC807 for heat-resistant superalloys (Inconel 718): rated S05–S20 by ISCAR.

The reasoning, step by step
  1. The situation

    Heat-resistant superalloys like Inconel are made to stay strong hot. They work-harden, conduct heat poorly so the heat piles up at the edge, and the hardened skin notches the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    The edge must cut sharp and positive and never dwell or rub, with a feed and depth that get under the last pass’s hardened layer, on a grade that stands the heat.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    A PVD grade: its thin coating keeps a tough, sharp edge, which is what makers recommend for sticky (smearing) materials and high-temperature alloys.

    Two sources: Sandvik Coromant and Seco Tools , sources [4, 5]

  4. So

    ISCAR rates IC807 (PVD-coated carbide) for S05–S20: Steel, austenitic stainless, high-temperature alloys and hard steel at moderate to fairly high speed, stable conditions.

    One source: ISCAR, the maker of the grade , sources [6]

  1. Sandvik Coromant — Workpiece materials: ISO S superalloys and titanium
  2. Mitsubishi Materials — Machining course: ISO group S, heat-resistant alloys
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  5. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  6. ISCAR — eCatalog grade data: IC807

Hardened · H

Read at H10, the centre of ISCAR’s H range (hardened steel). Each grade is one its own maker rates for H10 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for H10
MakerGradeTypeCoatingMaker’s rangeSource
KennametalKC5010PVD-coated carbidePVD, AlTiNH10–H10

One source: Kennametal, its own catalog

SecoTH1000PVD-coated carbidePVD, Ti-Al-Si-N nanolaminateabout H05–H15

One source: Seco Tools, its own catalog

Why IC807 for hardened steel

IC807 for hardened steel: rated H05–H15 by ISCAR.

The reasoning, step by step
  1. The situation

    Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    ISCAR rates IC807 (PVD-coated carbide) for H05–H15: Steel, austenitic stainless, high-temperature alloys and hard steel at moderate to fairly high speed, stable conditions.

    One source: ISCAR, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO H hardened steel
  2. Mitsubishi Materials — Machining course: ISO group H, hardened steel
  3. ISCAR — eCatalog grade data: IC807

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC807 at P10, P20, M10, S01, S10. ISCAR’s own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)