ISCAR · cermet
IC30N insert grade
IC30N is ISCAR’s cermet grade (Uncoated) for ISO P10–P30, M10–M20 and H10–H25, as ISCAR’s catalog prints it. Cermet for semi-finishing and finishing at high speed, medium feed.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- cermet
- Coating
- Uncoated
- ISO P
- P10–P30 · steel
- ISO M
- M10–M20 · stainless steel
- ISO H
- H10–H25 · hardened steel
- Operations
- turning, milling
IC30N equivalents by material
Steel · P
Read at P20, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM15 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P20–P25 | One source: Kennametal, its own catalog |
| Mitsubishi | MP3025 | cermet | PVD, Ti compound | P15–P35 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1525 | cermet | PVD | P05–P25 (core P15) | One source: Sandvik Coromant, its own catalog |
| Seco | TP1030 | cermet | PVD, Ti-Al-Si-N nanolaminate | about P10–P20 | One source: Seco Tools, its own catalog |
Why IC30N for steel
IC30N for steel: rated P10–P30 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC30N (cermet) for P10–P30: Cermet for semi-finishing and finishing at high speed, medium feed.
One source: ISCAR, the maker of the grade , sources [3]
Stainless · M
Read at M15, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | K313 | uncoated carbide | Uncoated | M10–M20 | One source: Kennametal, its own catalog |
| Mitsubishi | AP25N | cermet | PVD | M05–M25 | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC1115 | PVD-coated carbide | PVD | M05–M25 (core M15) | One source: Sandvik Coromant, its own catalog |
| Seco | TM1501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M10–M20 | One source: Seco Tools, its own catalog |
Why IC30N for austenitic stainless (304, 316)
IC30N for austenitic stainless (304, 316): rated M10–M20 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC30N (cermet) for M10–M20: Cermet for semi-finishing and finishing at high speed, medium feed.
One source: ISCAR, the maker of the grade , sources [4]
Hardened · H
Read at H20, the centre of ISCAR’s H range (hardened steel). Each grade is one its own maker rates for H20 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
No other maker’s verified grade covers H20 yet.
Why IC30N for hardened steel
IC30N for hardened steel: rated H10–H25 by ISCAR.
The reasoning, step by step
The situation
Hardened steel is hard and abrasive and makes heat; the edge needs hot hardness, and the tool, workholding and machine must be rigid.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
ISCAR rates IC30N (cermet) for H10–H25: Cermet for semi-finishing and finishing at high speed, medium feed.
One source: ISCAR, the maker of the grade , sources [3]
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC30N at P10, P20, P30, M10, M20. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)