Mitsubishi · cermet

AP25N insert grade

AP25N is Mitsubishi’s cermet grade (PVD) for ISO P05–P25, M05–M25 and K05–K25, as Mitsubishi’s catalog prints it. PVD-coated cermet for steel, stainless and cast iron finishing.

One source: Mitsubishi Materials, its own catalog

The cutting edge of a cermet insert in section: the cermet substrate, uncoated; rated for ISO P, M and K.cutting edgesubstrate cermetISO groupPMK
The edge in section; its ISO groups. Not to scale.

What Mitsubishi prints

Type
cermet
Coating
PVD
ISO P
P05–P25 · steel
ISO M
M05–M25 · stainless steel
ISO K
K05–K25 · cast iron
Operations
turning
Twin
VP25N (PVD): Mitsubishi prints the same range and use

Source: Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

AP25N equivalents by material

Steel · P

Read at P15, the centre of Mitsubishi’s P range (steel). Each grade is one its own maker rates for P15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC30NcermetUncoatedP10–P30

One source: ISCAR, its own catalog

KennametalKC5010PVD-coated carbidePVD, AlTiNP10–P20

One source: Kennametal, its own catalog

SandvikGC1525cermetPVDP05–P25 (core P15)

One source: Sandvik Coromant, its own catalog

SecoTP1030cermetPVD, Ti-Al-Si-N nanolaminateabout P10–P20

One source: Seco Tools, its own catalog

Why AP25N for steel

AP25N for steel: rated P05–P25 by Mitsubishi.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Mitsubishi rates AP25N (cermet) for P05–P25: PVD-coated cermet for steel, stainless and cast iron finishing.

    One source: Mitsubishi Materials, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

Stainless · M

Read at M15, the centre of Mitsubishi’s M range (stainless steel). Each grade is one its own maker rates for M15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for M15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC30NcermetUncoatedM10–M20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedM10–M20

One source: Kennametal, its own catalog

SandvikGC1115PVD-coated carbidePVDM05–M25 (core M15)

One source: Sandvik Coromant, its own catalog

SecoTM1501CVD-coated carbideCVD, Ti(C,N) + Al2O3, chrome used-edge detection layerabout M10–M20

One source: Seco Tools, its own catalog

Why AP25N for austenitic stainless (304, 316)

AP25N for austenitic stainless (304, 316): rated M05–M25 by Mitsubishi.

The reasoning, step by step
  1. The situation

    Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. What that means

    A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.

    Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]

  3. So

    Mitsubishi rates AP25N (cermet) for M05–M25: PVD-coated cermet for steel, stainless and cast iron finishing.

    One source: Mitsubishi Materials, the maker of the grade , sources [4]

  1. Sandvik Coromant — Workpiece materials: ISO M stainless
  2. Mitsubishi Materials — Machining course: ISO group M, stainless steel
  3. NeoNickel — Machining NeoNickel high performance alloys (archived May 18, 2026)
  4. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

Cast iron · K

Read at K15, the centre of Mitsubishi’s K range (cast iron). Each grade is one its own maker rates for K15 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for K15
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC20uncoated carbideUncoatedK10–K20

One source: ISCAR, its own catalog

KennametalK313uncoated carbideUncoatedK05–K20

One source: Kennametal, its own catalog

SandvikH13Auncoated carbideUncoatedK10–K30 (core K20)

One source: Sandvik Coromant, its own catalog

Why AP25N for gray cast iron

AP25N for gray cast iron: rated K05–K25 by Mitsubishi.

The reasoning, step by step
  1. The situation

    Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    Mitsubishi rates AP25N (cermet) for K05–K25: PVD-coated cermet for steel, stainless and cast iron finishing.

    One source: Mitsubishi Materials, the maker of the grade , sources [3]

  1. Sandvik Coromant — Workpiece materials: ISO K cast iron
  2. Mitsubishi Materials — Machining course: ISO group K, cast iron
  3. Mitsubishi Materials — General Catalog C010A, turning inserts: grades (pp. A034–A044) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a compilation across makers, lists AP25N at P01, P10, P20, M10, M20, K01, K10, K20. Mitsubishi Materials’ own catalog is the authority for its grade.

Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)