ISCAR · CVD-coated carbide
IC4050 insert grade
IC4050 is ISCAR’s CVD-coated carbide grade (CVD, TiCN + Al2O3 + TiN) for ISO P20–P50, M20–M30 and K20–K40, as ISCAR’s catalog prints it. Alloy steel, stainless and cast iron, interrupted cuts.
One source: ISCAR, its own catalog
What ISCAR prints
- Type
- CVD-coated carbide
- Coating
- CVD, TiCN + Al2O3 + TiN
- ISO P
- P20–P50 · steel
- ISO M
- M20–M30 · stainless steel
- ISO K
- K20–K40 · cast iron
- Operations
- turning, milling
IC4050 equivalents by material
Steel · P
Read at P35, the centre of ISCAR’s P range (steel). Each grade is one its own maker rates for P35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Mitsubishi | MC6125 | CVD-coated carbide | CVD, Accumulated TiCN-Al2O3-Ti compound, thick | P10–P35 (core P20) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC4335 | CVD-coated carbide | CVD | P25–P45 (core P35) | One source: Sandvik Coromant, its own catalog |
Why IC4050 for steel
IC4050 for steel: rated P20–P50 by ISCAR.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
ISCAR rates IC4050 (CVD-coated carbide) for P20–P50: Alloy steel, stainless and cast iron, interrupted cuts.
One source: ISCAR, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC4050
Stainless · M
Read at M25, the centre of ISCAR’s M range (stainless steel). Each grade is one its own maker rates for M25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | M20–M30 | One source: Kennametal, its own catalog |
| Mitsubishi | MC7025 | CVD-coated carbide | CVD, TiCN-Al2O3-TiN, thin | M20–M40 (core M30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | GC2025 | CVD-coated carbide | CVD | M15–M35 (core M25) | One source: Sandvik Coromant, its own catalog |
| Seco | TM2501 | CVD-coated carbide | CVD, Ti(C,N) + Al2O3, chrome used-edge detection layer | about M20–M25 | One source: Seco Tools, its own catalog |
Why IC4050 for austenitic stainless (304, 316)
IC4050 for austenitic stainless (304, 316): rated M20–M30 by ISCAR.
The reasoning, step by step
The situation
Austenitic stainless work-hardens as it is cut, conducts heat poorly and sticks to the edge. The hardened skin and chips wear a notch in the edge at the depth-of-cut line.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
What that means
A work-hardening alloy needs a sharp, positive edge, and a feed and depth that cut under the layer the last pass hardened. An edge that rubs hardens the next layer.
Two sources: Mitsubishi Materials and NeoNickel , sources [2, 3]
So
ISCAR rates IC4050 (CVD-coated carbide) for M20–M30: Alloy steel, stainless and cast iron, interrupted cuts.
One source: ISCAR, the maker of the grade , sources [4]
Cast iron · K
Read at K30, the centre of ISCAR’s K range (cast iron). Each grade is one its own maker rates for K30 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| Kennametal | KC5025 | PVD-coated carbide | PVD, AlTiN | K20–K30 | One source: Kennametal, its own catalog |
| Mitsubishi | UTi20T | uncoated carbide | Uncoated | K20–K35 (core K30) | One source: Mitsubishi Materials, its own catalog |
| Sandvik | H13A | uncoated carbide | Uncoated | K10–K30 (core K20) | One source: Sandvik Coromant, its own catalog |
Why IC4050 for gray cast iron
IC4050 for gray cast iron: rated K20–K40 by ISCAR.
The reasoning, step by step
The situation
Gray iron breaks into short chips (its graphite acts as a chipbreaker), but the hard particles in it are abrasive to the edge.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
ISCAR rates IC4050 (CVD-coated carbide) for K20–K40: Alloy steel, stainless and cast iron, interrupted cuts.
One source: ISCAR, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO K cast iron
- Mitsubishi Materials — Machining course: ISO group K, cast iron
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- ISCAR — eCatalog grade data: IC4050
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists IC4050 at P30, M30, K30. ISCAR’s own catalog is the authority for its grade.
It agrees with ISCAR’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)