Sandvik · CVD-coated carbide

GC4325 insert grade

GC4325 is Sandvik’s CVD-coated carbide grade (CVD) for ISO P10–P40, as Sandvik’s catalog prints it. Steel and steel castings, finishing to roughing; continuous and interrupted cuts at high metal removal rates, a broad application area.

One source: Sandvik Coromant, its own catalog

The cutting edge of a CVD-coated carbide insert in section: the carbide substrate under its CVD coating; rated for ISO P.cutting edgecoating CVDsubstrate carbideISO groupP
The edge in section; its ISO groups. Not to scale; the coating drawn thicker.

What Sandvik prints

Type
CVD-coated carbide
Coating
CVD
ISO P
P10–P40 (core P25) · steel
Operations
turning

Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

GC4325 equivalents by material

ISO P (steel)

Read at P25, the centre of Sandvik’s P range (steel). Each grade is one its own maker rates for P25 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.

Other makers’ grades rated for P25
MakerGradeTypeCoatingMaker’s rangeSource
ISCARIC8250CVD-coated carbideCVD, TiCN + Al2O3 + TiNP10–P35

One source: ISCAR, its own catalog

KennametalKCM15CVD-coated carbideCVD, Multilayer MTCVD TiCN-Al2O3P20–P25

One source: Kennametal, its own catalog

MitsubishiMC6125CVD-coated carbideCVD, Accumulated TiCN-Al2O3-Ti compound, thickP10–P35 (core P20)

One source: Mitsubishi Materials, its own catalog

Why GC4325 for steel

GC4325 for steel: rated P10–P40 (core P25) by Sandvik.

The reasoning, step by step
  1. The situation

    Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.

    Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]

  2. So

    A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.

    Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]

  3. So

    Sandvik rates GC4325 (CVD-coated carbide) for P10–P40 (core P25): Steel and steel castings, finishing to roughing; continuous and interrupted cuts at high metal removal rates, a broad application area.

    One source: Sandvik Coromant, the maker of the grade , sources [5]

  1. Sandvik Coromant — Workpiece materials: ISO P steel
  2. Mitsubishi Materials — Machining course: ISO group P, steel
  3. Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
  4. Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
  5. Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)

What the cross-reference says

Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC4325 at P10, P20, P30. Sandvik Coromant’s own catalog is the authority for its grade.

It agrees with Sandvik Coromant’s catalog.