Sandvik · CVD-coated carbide
GC4335 insert grade
GC4335 is Sandvik’s CVD-coated carbide grade (CVD) for ISO P25–P45, as Sandvik’s catalog prints it. Steel turning in tough, demanding cuts: difficult surfaces, vibration, heavy interruptions and unstable conditions.
One source: Sandvik Coromant, its own catalog
What Sandvik prints
- Type
- CVD-coated carbide
- Coating
- CVD
- ISO P
- P25–P45 (core P35) · steel
- Operations
- turning
Source: Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
GC4335 equivalents by material
ISO P (steel)
Read at P35, the centre of Sandvik’s P range (steel). Each grade is one its own maker rates for P35 in its own catalog, the same coating type first. Equivalent means the same ISO class, not the same cutting data.
| Maker | Grade | Type | Coating | Maker’s range | Source |
|---|---|---|---|---|---|
| ISCAR | IC4050 | CVD-coated carbide | CVD, TiCN + Al2O3 + TiN | P20–P50 | One source: ISCAR, its own catalog |
| Kennametal | KCM25 | CVD-coated carbide | CVD, Multilayer MTCVD TiCN-Al2O3 | P35–P45 | One source: Kennametal, its own catalog |
| Mitsubishi | MC6125 | CVD-coated carbide | CVD, Accumulated TiCN-Al2O3-Ti compound, thick | P10–P35 (core P20) | One source: Mitsubishi Materials, its own catalog |
Why GC4335 for steel
GC4335 for steel: rated P25–P45 (core P35) by Sandvik.
The reasoning, step by step
The situation
Steel makes chips that are fairly easy to control. The edge’s main enemy is heat, and the harder or higher in carbon the steel, the hotter the edge runs.
Two sources: Sandvik Coromant and Mitsubishi Materials , sources [1, 2]
So
A CVD grade: its thick coating, with an alumina layer that acts as a heat barrier, is what makers recommend for steel and cast iron.
Two sources: Sandvik Coromant and Seco Tools , sources [3, 4]
So
Sandvik rates GC4335 (CVD-coated carbide) for P25–P45 (core P35): Steel turning in tough, demanding cuts: difficult surfaces, vibration, heavy interruptions and unstable conditions.
One source: Sandvik Coromant, the maker of the grade , sources [5]
- Sandvik Coromant — Workpiece materials: ISO P steel
- Mitsubishi Materials — Machining course: ISO group P, steel
- Sandvik Coromant — Cutting tool materials (archived Oct 9, 2026)
- Seco Tools — A guide to insert coating processes and materials (D. Graham, Production Machining) (archived Jan 17, 2025)
- Sandvik Coromant — Turning Tools 2020 catalogue, grade descriptions (pp. A293–A298) (archived Nov 15, 2026)
What the cross-reference says
Mitsubishi’s grade comparison table, a competitor’s compilation, lists GC4335 at P30, P40. Sandvik Coromant’s own catalog is the authority for its grade.
It agrees with Sandvik Coromant’s catalog.
Source: Mitsubishi Materials USA — Grades Comparison Table (archived Jul 16, 2024)